NM2 - CuNi7Zn39Pb3Mn2 - CW400J

Want to keep this datasheet? Save it now in your required format

Description

Nickel silver specially developed for free machining, designed and manufactured by Lebronze alloys.

Related Standards

This material data has been provided by Lebronze Alloys.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.4 g/cm³

Show Supplier Material materials with Density of 8.4 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

115 GPa

Show Supplier Material materials with Elastic modulus of 115 GPa

Elongation

23.0 °C

3 - 38 %

Show Supplier Material materials with Elongation of 3 - 38 %

Hardness, Brinell

23.0 °C

103 - 216 [-]

Show Supplier Material materials with Hardness, Brinell of 103 - 216 [-]

Hardness, Rockwell C

23.0 °C

0 - 19 [-]

Show Supplier Material materials with Hardness, Rockwell C of 0 - 19 [-]

Hardness, Vickers

23.0 °C

110 - 175 [-]

Show Supplier Material materials with Hardness, Vickers of 110 - 175 [-]

Tensile strength

23.0 °C

490 - 780 MPa

Show Supplier Material materials with Tensile strength of 490 - 780 MPa

Yield strength

23.0 °C

240 - 700 MPa

Show Supplier Material materials with Yield strength of 240 - 700 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.9E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.9E-5 1/K

for 20-200°C

Thermal conductivity

23.0 °C

33 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 33 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

4.00E+6 S/m

Show Supplier Material materials with Electrical conductivity of 4.00E+6 S/m

Specific Electrical conductivity

7 % IACS

Show Supplier Material materials with Specific Electrical conductivity of 7 % IACS

Technological properties

Property
Application areas

writing instruments screws fiber optic connectors spare parts for eyeglasses jewellery

General machinability

90 %