Description

Constantan 45 is a resistance non-magnetic alloy (Copper Nickel Manganese) designed and manufacturing by Lebronze alloys (ex. CLAL, CLAL MSX). It is available in rolled products (strip, sheets…) and drawn products (wires, rods).


Its main advantages and properties are:
  • High resistivity and stability of electrical resistance
  • Low temperature coefficient of resistance
  • Excellent resistance to oxidation and corrosion
  • Good working properties, excellent weldability and solderability
  • Equivalent Materials

    This material data has been provided by Lebronze Alloys.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyTemperatureValue

    Density

    23.0 °C

    8.9 g/cm³

    Show Supplier Material materials with Density of 8.9 g/cm³

    Thermal

    PropertyTemperatureValue

    Thermal conductivity

    23.0 °C

    23 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 23 W/(m·K)

    Electrical

    PropertyTemperatureValueComment

    Electrical resistivity

    23.0 °C

    4.9E-7 Ω·m

    Show Supplier Material materials with Electrical resistivity of 4.9E-7 Ω·m

    Temperature coefficient of resistance

    -20.0 °C

    -8E-5 1/K

    Show Supplier Material materials with Temperature coefficient of resistance of -8E-5 1/K

    between -20 and +150°C

    150.0 °C

    4E-5 1/K

    Show Supplier Material materials with Temperature coefficient of resistance of 4E-5 1/K

    between -20 and +150°C

    Themo EMF

    23.0 °C

    -4E-5 V/K

    Show Supplier Material materials with Themo EMF of -4E-5 V/K

    against copper

    Technological properties

    Property
    Application areas

    Resistors - Electrical shunts - Heating elements - Thermocouples