Niclal 42 (Strips, Rods, Wires) - CuMn11Ni4

Want to keep this datasheet? Save it now in your required format

Description

Niclal42 is a Copper Manganese Nickel alloy with high precision resistance and resistance stability. It is designed and manufactured by Lebronze alloys (ex. CLAL, CLAL MSX). It shows the following features and properties:


  • High stability of electrical resistance (42 μohm.cm)
  • Good working properties
  • Excellent weldability
  • Equivalent Materials

    This material data has been provided by Lebronze Alloys.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyTemperatureValue

    Density

    23.0 °C

    8.76 g/cm³

    Show Supplier Material materials with Density of 8.76 g/cm³

    Thermal

    PropertyTemperatureValueComment

    Coefficient of thermal expansion

    23.0 °C

    1.8E-5 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 1.8E-5 1/K

    for 20-200°C

    Thermal conductivity

    23.0 °C

    22 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 22 W/(m·K)

    Electrical

    PropertyTemperatureValue

    Electrical resistivity

    23.0 °C

    4.2E-7 Ω·m

    Show Supplier Material materials with Electrical resistivity of 4.2E-7 Ω·m

    Technological properties

    Property
    Application areas

    Precision resistors / Electrical shunts in electricity meters / Electrical shunts in DC ammeters