General
Property | Value | Temperature |
---|---|---|
Density | 8.76 g/cm³ Show Supplier Material materials with Density of 8.76 g/cm³ at 23.0 °C | 23.0 °C |
Thermal
Property | Value | Temperature | Comment |
---|---|---|---|
Coefficient of thermal expansion | 1.8E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.8E-5 1/K at 23.0 °C | 23.0 °C | for 20-200°C |
Thermal conductivity | 22 W/(m·K) Show Supplier Material materials with Thermal conductivity of 22 W/(m·K) at 23.0 °C | 23.0 °C |
Electrical
Property | Value | Temperature | Comment |
---|---|---|---|
Electrical resistivity | 4.3E-7 Ω·m Show Supplier Material materials with Electrical resistivity of 4.3E-7 Ω·m at 23.0 °C | 23.0 °C | |
Temperature coefficient of resistance | -1.5E-5 1/K Show Supplier Material materials with Temperature coefficient of resistance of -1.5E-5 1/K at -20.0 °C | -20.0 °C | between -20 and +150°C |
1.5E-5 1/K Show Supplier Material materials with Temperature coefficient of resistance of 1.5E-5 1/K at 150.0 °C | 150.0 °C | between -20 and +150°C | |
Themo EMF | -9.8E-7 V/K Show Supplier Material materials with Themo EMF of -9.8E-7 V/K at 23.0 °C | 23.0 °C | against copper |
Technological properties
Property | ||
---|---|---|
Application areas | Precision resistors - Electrical shunts in electricity meter - Electrical shunts in DC ammeters |