Thermoplastic elastomer TPU reinforced with 20% long glass fiber, general grade. The key features are:


  • High toughness
  • High rigidity
  • Low water absorption
  • High dimensional stability
  • Chemical resistance
  • Good product resistance
  • Ashby charts

    See where TPU LGF20 LFT-G® falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    Density

    ρ

    1.33 g/cm³ at 23 °C

    ASTM D792

    Mechanical

    Elastic modulus

    E

    6.9 GPa at 23 °C

    Show Thermoplastic Polyurethane (TPU) materials with Elastic modulus of 6.9 GPa at 23 °C

    ASTM D638

    Elongation

    A

    2 - 3 % at 23 °C

    Show Thermoplastic Polyurethane (TPU) materials with Elongation of 2 - 3 % at 23 °C

    ASTM D638

    Flexural modulus

    Ebend

    6.21 GPa at 23 °C

    Show Thermoplastic Polyurethane (TPU) materials with Flexural modulus of 6.21 GPa at 23 °C

    ASTM D790

    Flexural strength

    σbend

    221 MPa at 23 °C

    Show Thermoplastic Polyurethane (TPU) materials with Flexural strength of 221 MPa at 23 °C

    ASTM D790

    Impact strength, Izod notched, ASTM

    IIzod,not,astm

    267 J/m at 23 °C

    Show Thermoplastic Polyurethane (TPU) materials with Impact strength, Izod notched, ASTM of 267 J/m at 23 °C

    ASTM D256

    Impact strength, Izod unnotched, ASTM

    IIzod,unnot,astm

    1175 J/m at 23 °C

    Show Thermoplastic Polyurethane (TPU) materials with Impact strength, Izod unnotched, ASTM of 1175 J/m at 23 °C

    ASTM D4812

    Tensile strength

    Rm

    145 MPa at 23 °C

    Show Thermoplastic Polyurethane (TPU) materials with Tensile strength of 145 MPa at 23 °C

    ASTM D638

    Thermal

    Flammability

    HB ASTM D635, for 1.5mm

    Heat deflection temperature, 1.80 MPa

    HDT1.8,MPa

    85 °C

    ASTM D648

    Rheological Properties

    Shrinkage

    cshrink

    0.1 - 0.2 % at 23 °C

    ASTM D955, (1/8 in (3.2 mm)section)

    Technological properties

    Application areas

    Car Doors and window, Mechanical parts, Pneumatic nail gun boxes, Nut and bolts, Fireman shoe parts (safety shoe parts)

    Color

    Black/white or custom color

    Filler Type

    Fillers

    20% Long Glass Fiber

    Processing Tag

    Processing methods

    Injection Moulding. Injection Pressure 69 - 103 MPa, Melt Temperature 221 - 243 °C, Mould temperature 52 - 93 °C, Pre-drying 6 hrs @ 107 °C, Moisture Content 0.01%, Dew Point -40°C

    This material data has been provided by Xiamen LFT Composite Plastic Co.,ltd.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.