PA6 GF60 LFT-G ®

Alternative and trade names
LFT-G® PA6-NA-LGF60, PA6-I-LGF60
Want to keep this datasheet? Save it now in your required format

Description

Nylon 6 (Polyamide 6) reinforced with 60% long glass fiber. the key features are:


  • High toughness (specially at low temperatures)
  • Excellent anti-creep and fatigure resistance
  • Low warpage
  • Impact modified and flame retadant grades are available
  • This material data has been provided by Xiamen LFT Composite Plastic Co.,ltd.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValueComment

    Density

    23.0 °C

    1.68 g/cm³

    Show Supplier Material materials with Density of 1.68 g/cm³

    ASTM D792

    Mechanical

    PropertyTemperatureValueComment

    Elastic modulus

    23.0 °C

    23.13 GPa

    Show Supplier Material materials with Elastic modulus of 23.13 GPa

    ASTM D638

    Elongation

    23.0 °C

    1.5 %

    Show Supplier Material materials with Elongation of 1.5 %

    ASTM D638

    Flexural modulus

    23.0 °C

    18.86 GPa

    Show Supplier Material materials with Flexural modulus of 18.86 GPa

    ASTM D790

    Flexural strength

    23.0 °C

    333 MPa

    Show Supplier Material materials with Flexural strength of 333 MPa

    ASTM D790

    Impact strength, Izod notched, ASTM

    23.0 °C

    316 J/m

    Show Supplier Material materials with Impact strength, Izod notched, ASTM of 316 J/m

    ASTM D256

    Tensile strength

    23.0 °C

    237 MPa

    Show Supplier Material materials with Tensile strength of 237 MPa

    ASTM D638

    Thermal

    PropertyValue

    Flammability

    HB ASTM D635, for 1.5mm

    Rheological Properties

    PropertyTemperatureValueComment

    Shrinkage

    23.0 °C

    0.1 - 0.2 %

    Show Supplier Material materials with Shrinkage of 0.1 - 0.2 %

    ASTM D955, (1/8 in (3.2 mm)section)

    Technological properties

    Property
    Application areas

    Sports equipment, Power tool housing, High-speed rail accessories, Water pump impeller, Washing machine drum, gears, Automotive: Spare wheel pan, Door module, Dashboard cross member, Seat pan, Bumper bracket, Front end

    Color

    Natural, and custom colors

    Fillers

    60% Long Glass Fiber

    Processing methods

    Injection Moulding. Injection Pressure 69 - 124 MPa, Melt Temperature 243 - 271 °C, Mould temperature 54 - 93 °C, Pre-drying 2 hrs @ 82 °C, Moisture Content 0.20%, Dew Point -29°C