ABS (Acrylonitrile Butadiene Styrene) reinforced with 30% long carbon fiber with high toughness and strength.

This material data has been provided by Xiamen LFT Composite Plastic Co.,ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.18 g/cm³

Show Supplier Material materials with Density of 1.18 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

14.52 GPa

Show Supplier Material materials with Elastic modulus of 14.52 GPa

ASTM D638

Elongation

23.0 °C

0.14 %

Show Supplier Material materials with Elongation of 0.14 %

ASTM D638

Flexural modulus

23.0 °C

37.61 GPa

Show Supplier Material materials with Flexural modulus of 37.61 GPa

ASTM D790

Flexural strength

23.0 °C

213.3 MPa

Show Supplier Material materials with Flexural strength of 213.3 MPa

ASTM D790

Impact strength, Izod notched, ASTM

23.0 °C

146.3 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 146.3 J/m

ASTM D256

Tensile strength

23.0 °C

109 MPa

Show Supplier Material materials with Tensile strength of 109 MPa

ASTM D638

Thermal

PropertyValue

Flammability

HB ASTM D635, for 1.5mm

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.1 - 0.3 %

Show Supplier Material materials with Shrinkage of 0.1 - 0.3 %

ASTM D955, (1/8 in (3.2 mm)section)

Technological properties

Property
Application areas

Used for automotive interior decoration, power tools, sports equipment, lawnmowers and snow blowers, industrial parts, office equipment housings, etc .

Color

Natural, and custom colors

Fillers

30% Long Carbon Fiber

Processing methods

Injection Moulding. Injection Pressure 70 - 110 MPa, Melt Temperature 210 - 240 °C, Mould temperature 60 - 90 °C, Pre-drying 2- 4 hrs @ 80 - 95 °C, Moisture Content 0.01%