TPU LGF30 LFT-G®

Alternative and trade names
LFT-G® TPU-NA-LGF30 , TPU-LGF30
Want to keep this datasheet? Save it now in your required format

Description

Thermoplastic elastomer TPU reinforced with 30% long glass fiber, general grade. The key features are:


  • High toughness
  • High rigidity
  • Low water absorption
  • High dimensional stability
  • Chemical resistance
  • Good product resistance
  • This material data has been provided by Xiamen LFT Composite Plastic Co.,ltd.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValueComment

    Density

    23.0 °C

    1.43 g/cm³

    Show Supplier Material materials with Density of 1.43 g/cm³

    ASTM D792

    Mechanical

    PropertyTemperatureValueComment

    Elastic modulus

    23.0 °C

    8.97 GPa

    Show Supplier Material materials with Elastic modulus of 8.97 GPa

    ASTM D638

    Elongation

    23.0 °C

    2 - 3 %

    Show Supplier Material materials with Elongation of 2 - 3 %

    ASTM D638

    Flexural modulus

    23.0 °C

    7.59 GPa

    Show Supplier Material materials with Flexural modulus of 7.59 GPa

    ASTM D790

    Flexural strength

    23.0 °C

    266 MPa

    Show Supplier Material materials with Flexural strength of 266 MPa

    ASTM D790

    Impact strength, Izod notched, ASTM

    23.0 °C

    363 J/m

    Show Supplier Material materials with Impact strength, Izod notched, ASTM of 363 J/m

    ASTM D256

    Impact strength, Izod unnotched, ASTM

    23.0 °C

    1228 J/m

    Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1228 J/m

    ASTM D4812

    Tensile strength

    23.0 °C

    186 MPa

    Show Supplier Material materials with Tensile strength of 186 MPa

    ASTM D638

    Thermal

    PropertyValueComment

    Heat deflection temperature, 1.80 MPa

    85 °C

    Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 85 °C

    ASTM D648

    Flammability

    HB ASTM D635, for 1.5mm

    Rheological Properties

    PropertyTemperatureValueComment

    Shrinkage

    23.0 °C

    0.1 - 0.2 %

    Show Supplier Material materials with Shrinkage of 0.1 - 0.2 %

    ASTM D955, (1/8 in (3.2 mm)section)

    Technological properties

    Property
    Application areas

    Car Doors and window, Mechanical parts, Pneumatic nail gun boxes, Nut and bolts, Fireman shoe parts (safety shoe parts)

    Color

    Natural/Also as required

    Fillers

    30% Long Glass Fiber

    Processing methods

    Injection Moulding. Injection Pressure 69 - 103 MPa, Melt Temperature 221 - 243 °C, Mould temperature 52 - 93 °C, Pre-drying 6 hrs @ 107 °C, Moisture Content 0.01%, Dew Point -40°C