PEEK LCF40 LFT-G®

Alternative and trade names
LFT-G® PEEK-NA-LCF40, PEEK-CF40
Want to keep this datasheet? Save it now in your required format

Description

Polyetherether Ketone (PEEK) reinforced with 40% carbon fiber. The key features are:


  • Heat and chemical resistance
  • Low friction coefficient
  • Good load bearing
  • This material data has been provided by Xiamen LFT Composite Plastic Co.,ltd.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValueComment

    Density

    23.0 °C

    1.45 g/cm³

    Show Supplier Material materials with Density of 1.45 g/cm³

    ASTM D792

    Mechanical

    PropertyTemperatureValueComment

    Elastic modulus

    23.0 °C

    37.89 GPa

    Show Supplier Material materials with Elastic modulus of 37.89 GPa

    ASTM D790

    Elongation

    23.0 °C

    0.7 %

    Show Supplier Material materials with Elongation of 0.7 %

    ASTM D638

    Flexural modulus

    23.0 °C

    25.39 GPa

    Show Supplier Material materials with Flexural modulus of 25.39 GPa

    ASTM D790

    Flexural strength

    23.0 °C

    304 MPa

    Show Supplier Material materials with Flexural strength of 304 MPa

    ASTM D790

    Impact strength, Izod unnotched, ASTM

    23.0 °C

    726 J/m

    Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 726 J/m

    ASTM D4812

    Tensile strength

    23.0 °C

    218 MPa

    Show Supplier Material materials with Tensile strength of 218 MPa

    ASTM D638

    Technological properties

    Property
    Application areas

    Drone rack, Drone wing, 5G communication, Bone External Fixator bracket, Marine propellers.

    Fillers

    40% Carbon Fiber

    Processing methods

    Injection Molding