General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 2.8 g/cm³ Show Supplier Material materials with Density of 2.8 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 103 GPa Show Supplier Material materials with Elastic modulus of 103 GPa |
Elongation | 23.0 °C | 7 % Show Supplier Material materials with Elongation of 7 % |
Poisson's ratio | 23.0 °C | 0.3 [-] Show Supplier Material materials with Poisson's ratio of 0.3 [-] |
Tensile strength | 23.0 °C | 470 MPa Show Supplier Material materials with Tensile strength of 470 MPa |
Yield strength Rp0.2 | 23.0 °C | 380 MPa Show Supplier Material materials with Yield strength Rp0.2 of 380 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.7E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.7E-5 1/K |
Melting point | 570 °C Show Supplier Material materials with Melting point of 570 °C | |
Specific heat capacity | 23.0 °C | 850 J/(kg·K) Show Supplier Material materials with Specific heat capacity of 850 J/(kg·K) |
Thermal conductivity | 23.0 °C | 150 W/(m·K) Show Supplier Material materials with Thermal conductivity of 150 W/(m·K) |
Technological properties
Property | ||
---|---|---|
Application areas | Commercial and Military Aerospace: Outlet guide vanes, Hydraulic / Fuel blocks, Wheels, Fixed wing structure/ skins, Helicopter components - Commercial and Preformance Automotive: Pistons, Piston pins, Cylinder liners, Brake calipers, Connecting rods, Push rods, Valve train, Chassis components - Space, Defence and Optical Systems: Optical systems & sensors, Satellite structures, Astronomical telescopes | |
Processing history | Precision Extrusion |