SABIC® FORTIFY™ C11075DF

Want to keep this datasheet? Save it now in your required format

Description

SABIC® FORTIFY™ C11075DF Ethylene octene copolymer produced by solution polymerization using metallocene catalyst for foaming SABIC® FORTIFY™ C11075DF is a grade typically used in foam application. This grade is designed as a low density and high performance copolymer modifier to provide superior resilience and compression set properties.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.87 g/cm³

Show Material materials with Density of 0.87 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

0.01 GPa

Show Material materials with Flexural modulus of 0.01 GPa

ASTM D790 A | (1% Secant)

Tear strength

23.0 °C

39 kN/m

Show Material materials with Tear strength of 39 kN/m

ASTM D624

Thermal

PropertyValueComment

Glass transition temperature

-52 °C

Show Material materials with Glass transition temperature of -52 °C

SABIC method

Melting point

62 °C

Show Material materials with Melting point of 62 °C

SABIC method

Rheological Properties

PropertyValueComment

Melt mass-flow rate

1 g/10min

Show Material materials with Melt mass-flow rate of 1 g/10min

ASTM D1238 | 190°C/2.16 kg

Technological properties

Property
Application areas

Footwear,Packaging,Automotive ,Foam