SABIC® FORTIFY™ C30070D

Want to keep this datasheet? Save it now in your required format

Description

SABIC® FORTIFY™ C30070D is an ethylene octene copolymer produced by solution polymerization using metallocene catalyst. This product is available as free flowing pellets. SABIC® FORTIFY™ C30070D is designed as a high performance copolymer modifier to provide superior toughness, softness and opticalproperties. It also provides excellent flow properties.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

0.868 g/cm³

Show Material materials with Density of 0.868 g/cm³

ASTM D792

Mechanical

PropertyValueComment

Flexural modulus

0.0108 GPa

Show Material materials with Flexural modulus of 0.0108 GPa

ASTM D790 A | (1% Secant)

Tear strength

29.4 kN/m

Show Material materials with Tear strength of 29.4 kN/m

ASTM D624

Thermal

PropertyValueComment

Glass transition temperature

-52.0 °C

Show Material materials with Glass transition temperature of -52.0 °C

SABIC method

Melting point

62.0 °C

Show Material materials with Melting point of 62.0 °C

SABIC method

Rheological Properties

PropertyValueComment

Mooney viscosity

2.0 MU

Show Material materials with Mooney viscosity of 2.0 MU

ASTM D1646 | ML 1+4, 121 °C

Technological properties

Property
Application areas

Wire & cable,Impact modification