Description

SABIC® FORTIFY™ C3080 is an ethylene octene copolymer produced by solution polymerization using metallocene catalyst. This product is available as free flowing pellets. SABIC® FORTIFY™ C3080 is designed as a high performance copolymer modifier to provide superior toughness, softness and optical properties. It provides excellent flow properties too.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

0.88 g/cm³

Show Material materials with Density of 0.88 g/cm³

ASTM D792

Mechanical

PropertyValueComment

Flexural modulus

0.019600000000000003 GPa

Show Material materials with Flexural modulus of 0.019600000000000003 GPa

ASTM D790 A | (1% Secant)

Tear strength

41.2 kN/m

Show Material materials with Tear strength of 41.2 kN/m

ASTM D624

Thermal

PropertyValueComment

Glass transition temperature

-49.0 °C

Show Material materials with Glass transition temperature of -49.0 °C

SABIC method

Melting point

68.0 °C

Show Material materials with Melting point of 68.0 °C

SABIC method

Rheological Properties

PropertyValueComment

Mooney viscosity

11.0 MU

Show Material materials with Mooney viscosity of 11.0 MU

ASTM D1646 | ML 1+4, 121 °C

Technological properties

Property
Application areas

Wire & cable,Impact modification