Common features of Hytrel® thermoplastic polyester elastomer include mechanical and physical properties such as exceptional toughness and resilience, high resistance to creep, impact and flex fatigue, flexibility at low temperatures and good retention of properties at elevated temperatures. In addition, it resists many industrial chemicals, oils and solvents. Special grades include heat stabilised, flame retardant, food contact compliant, blow molding and extrusion grades. Concentrates offered include black pigments, UV protection additives, heat stabilisers, and flame retardants. Hytrel® thermoplastic polyester elastomer is plasticiser free.The good melt stability of Hytrel® thermoplastic polyester elastomer normally enables the recycling of properly handled production waste. If recycling is not possible, DuPont recommends, as the preferred option, incineration with energy recovery (-24 kJ/g of base polymer) in appropriately equipped installations.For disposal, local regulations have to be observed. Hytrel® thermoplastic polyester elastomer typically is used in demanding applications in the automotive, fluid power, electrical/electronic, consumer goods, appliance and power tool, sporting goods, furniture, industrial and off-road transportation/equipment industry.Hytrel® 40CB is a black master batch which can provide improved UV resistance when blended with other Hytrel® grades.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Thermal

PropertyValueComment

Melting point

154 °C

Show Material materials with Melting point of 154 °C

ISO 11357-1/-3 | 18°F/min

Flammability

FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

300 V

Show Material materials with Comparative tracking index of 300 V

IEC 60112

Dielectric strength

23.0 °C

34 kV/mm

Show Material materials with Dielectric strength of 34 kV/mm

IEC 60243-1

Dissipation factor, 100Hz

23.0 °C

6E-3 [-]

Show Material materials with Dissipation factor, 100Hz of 6E-3 [-]

IEC 62631-2-1

Dissipation factor, 1MHz

23.0 °C

0.01 [-]

Show Material materials with Dissipation factor, 1MHz of 0.01 [-]

IEC 62631-2-1

Volume resistivity

23.0 °C

1.00E+15 Ω·cm

Show Material materials with Volume resistivity of 1.00E+15 Ω·cm

min. | IEC 62631-3-1

Technological properties

Property
Fillers

Carbon Black

Processing methods

Drying Recommended: yes