Hytrel® G3548 NC010

Alternative and trade names
TPC-ET
Want to keep this datasheet? Save it now in your required format

Description

Common features of Hytrel® thermoplastic polyester elastomer include mechanical and physical properties such as exceptional toughness and resilience, high resistance to creep, impact and flex fatigue, flexibility at low temperatures and good retention of properties at elevated temperatures. In addition, it resists many industrial chemicals, oils and solvents. Special grades include heat stabilised, flame retardant, food contact compliant, blow molding and extrusion grades. Concentrates offered include black pigments, UV protection additives, heat stabilisers, and flame retardants. Hytrel® thermoplastic polyester elastomer is plasticiser free.The good melt stability of Hytrel® thermoplastic polyester elastomer normally enables the recycling of properly handled production waste. If recycling is not possible, DuPont recommends, as the preferred option, incineration with energy recovery (-24 kJ/g of base polymer) in appropriately equipped installations.For disposal, local regulations have to be observed. Hytrel® thermoplastic polyester elastomer typically is used in demanding applications in the automotive, fluid power, electrical/electronic, consumer goods, appliance and power tool, sporting goods, furniture, industrial and off-road transportation/equipment industry.Hytrel® G3548 is a low modulus grade with nominal hardness of 35D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injection molding and extrusion.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.15 g/cm³

Show Material materials with Density of 1.15 g/cm³

ISO 1183

Water absorption

23.0 °C

6.9 %

Show Material materials with Water absorption of 6.9 %

Sim. to ISO 62 | Immersion 24h

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

0.03 GPa

Show Material materials with Elastic modulus of 0.03 GPa

ISO 527-1/-2

Elongation

23.0 °C

200 %

Show Material materials with Elongation of 200 %

ISO 527-1/-2 | 50mm/min

Flexural modulus

23.0 °C

0.03 GPa

Show Material materials with Flexural modulus of 0.03 GPa

ISO 178

Hardness, Shore D

23.0 °C

24 [-]

Show Material materials with Hardness, Shore D of 24 [-]

ISO 7619-1 | 15 seconds

Tear strength

23.0 °C

60 kN/m

Show Material materials with Tear strength of 60 kN/m

ISO 34-1

Tear strength, transverse

23.0 °C

80 kN/m

Show Material materials with Tear strength, transverse of 80 kN/m

ISO 34-1

Tensile strength

23.0 °C

10 MPa

Show Material materials with Tensile strength of 10 MPa

ISO 527-1/-2 | 50mm/min

Impact strength, Charpy notched

No Break @ 23,-6,-40°C, ISO 179/1eA

Impact strength, Izod unnotched

No Break @ -40°C, ISO 180/1A

Thermal

PropertyValueComment

Glass transition temperature

-45 °C

Show Material materials with Glass transition temperature of -45 °C

ISO 11357-1/-2 | 18°F/min

Melting point

157 °C

Show Material materials with Melting point of 157 °C

ISO 11357-1/-3 | 18°F/min

Relative temperature index, electrical

50 °C

Show Material materials with Relative temperature index, electrical of 50 °C

UL 746B | 120mil

Relative temperature index, mechanical impact

50 °C

Show Material materials with Relative temperature index, mechanical impact of 50 °C

UL 746B | 120mil

Relative temperature index, mechanical strength

50 °C

Show Material materials with Relative temperature index, mechanical strength of 50 °C

UL 746B | 120mil

Vicat softening temperature

70 °C

Show Material materials with Vicat softening temperature of 70 °C

ISO 306 | 90°F, 2 lbf

Flammability

Burning Behav. at 60mil nom. thickn.: HB class, Thickness tested: 1.5 mm, UL recognition: yes -, Burning Behav. at thickness h: HB class, Thickness tested: 3 mm, UL recognition: yes -, FMVSS Class: B -, Burning rate, Thickness 1 mm: 52 mm/min

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

10 g/10min

Show Material materials with Melt mass-flow rate of 10 g/10min

ISO 1133 | 190°C/2.16kg

Shrinkage

23.0 °C

0.8 %

Show Material materials with Shrinkage of 0.8 %

ISO 294-4, 2577

Shrinkage, transverse

23.0 °C

0.8 %

Show Material materials with Shrinkage, transverse of 0.8 %

ISO 294-4, 2577

Technological properties

Property
Processing methods

Drying Recommended: yes, Drying Temperature: 90°C, Drying Time, Dehumidified Dryer: 2-3h, Processing Moisture Content: ≤0.08%, Melt Temperature Optimum: 190°C, Min. melt temperature: 180°C, Max. melt temperature: 200°C, Mold Temperature Optimum: 40°C, Min. mold temperature: 30°C, Max. mold temperature: 40°C