Hytrel® RS 40F3 NC010

Alternative and trade names
TPC-ET
Want to keep this datasheet? Save it now in your required format

Description

Common features of Hytrel® thermoplastic polyester elastomer include mechanical and physical properties such as exceptional toughness and resilience, high resistance to creep, impact and flex fatigue, flexibility at low temperatures and good retention of properties at elevated temperatures. In addition, it resists many industrial chemicals, oils and solvents. Special grades include heat stabilised, flame retardant, food contact compliant, blow molding and extrusion grades. Concentrates offered include black pigments, UV protection additives, heat stabilisers, and flame retardants.Hytrel® thermoplastic polyester elastomer is plasticiser free.The good melt stability of Hytrel® thermoplastic polyester elastomer normally enables the recycling of properly handled production waste. If recycling is not possible, DuPont recommends, as the preferred option, incineration with energy recovery (-24 kJ/g of base polymer) in appropriately equipped installations.For disposal, local regulations have to be observed.Hytrel® thermoplastic polyester elastomer typically is used in demanding applications in the automotive, fluid power, electrical/electronic, consumer goods, appliance and power tool, sporting goods, furniture, industrial and off-road transportation/equipment industry.Hytrel® RS 40F3 NC010 is a high flow, low modulus grade containing at least 50% renewably sourced ingredients by weight. It is suitable for injection molding processes.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.11 g/cm³

Show Material materials with Density of 1.11 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

0.05 GPa

Show Material materials with Elastic modulus of 0.05 GPa

ISO 527-1/-2

Elongation

23.0 °C

800 %

Show Material materials with Elongation of 800 %

ISO 527-1/-2

Flexural modulus

23.0 °C

0.05 GPa

Show Material materials with Flexural modulus of 0.05 GPa

ISO 178

Hardness, Shore D

23.0 °C

37 [-]

Show Material materials with Hardness, Shore D of 37 [-]

max., ISO 7619-1

Tear strength

23.0 °C

97 kN/m

Show Material materials with Tear strength of 97 kN/m

ISO 34-1

Tear strength, transverse

23.0 °C

99 kN/m

Show Material materials with Tear strength, transverse of 99 kN/m

ISO 34-1

Tensile strength

23.0 °C

26 MPa

Show Material materials with Tensile strength of 26 MPa

ISO 527-1/-2

Impact strength, Charpy notched

No Break @ 23,-6°C, ISO 179/1eA

Impact strength, Charpy unnotched

No Break @ 23,-6°C, ISO 179/1eA

Thermal

PropertyTemperatureValueComment

Brittleness temperature

-90 °C

Show Material materials with Brittleness temperature of -90 °C

ISO 974

Coefficient of thermal expansion

23.0 °C

2.1E-4 1/K

Show Material materials with Coefficient of thermal expansion of 2.1E-4 1/K

ISO 11359-1/-2

Coefficient of thermal expansion, transverse

23.0 °C

2E-4 1/K

Show Material materials with Coefficient of thermal expansion, transverse of 2E-4 1/K

ISO 11359-1/-2

Heat deflection temperature, 0.45 MPa

50 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 50 °C

ISO 75-1/-2

Melting point

190 °C

Show Material materials with Melting point of 190 °C

ISO 11357-1/-3 | 18°F/min

Thermal diffusivity

23.0 °C

0 mm²/s

Show Material materials with Thermal diffusivity of 0 mm²/s

Vicat softening temperature

126 °C

Show Material materials with Vicat softening temperature of 126 °C

ISO 306 | 90°F, 2 lbf

Flammability

Burning Behav. at 60mil nom. thickn.: HB class, Thickness tested: 1.5 mm, Oxygen index: 20 %, FMVSS Class: SE -

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

20 g/10min

Show Material materials with Melt mass-flow rate of 20 g/10min

ISO 1133 | 220°C/2.16kg

Melt volume-flow rate

20 cm³/10min

Show Material materials with Melt volume-flow rate of 20 cm³/10min

ISO 1133

Shrinkage

23.0 °C

0.8 %

Show Material materials with Shrinkage of 0.8 %

ISO 294-4, 2577

Shrinkage, transverse

23.0 °C

0.6 %

Show Material materials with Shrinkage, transverse of 0.6 %

ISO 294-4, 2577

Technological properties

Property
Processing methods

Drying Recommended: yes, Drying Temperature: 100°C, Drying Time, Dehumidified Dryer: 2-3h, Processing Moisture Content: ≤0.08%, Melt Temperature Optimum: 225°C, Min. melt temperature: 220°C, Max. melt temperature: 250°C, Mold Temperature Optimum: 40°C, Min. mold temperature: 30°C, Max. mold temperature: 40°C