Hytrel® SC988 NC010

Alternative and trade names
TPC-ET
Want to keep this datasheet? Save it now in your required format

Description

Common features of Hytrel® thermoplastic polyester elastomer include mechanical and physical properties such as exceptional toughness and resilience, high resistance to creep, impact and flex fatigue, flexibility at low temperatures and good retention of properties at elevated temperatures. In addition, it resists many industrial chemicals, oils and solvents. Special grades include heat stabilised, flame retardant, food contact compliant, blow molding and extrusion grades. Concentrates offered include black pigments, UV protection additives, heat stabilisers, and flame retardants. Hytrel® thermoplastic polyester elastomer is plasticiser free.The good melt stability of Hytrel® thermoplastic polyester elastomer normally enables the recycling of properly handled production waste. If recycling is not possible, DuPont recommends, as the preferred option, incineration with energy recovery (-24 kJ/g of base polymer) in appropriately equipped installations.For disposal, local regulations have to be observed. Hytrel® thermoplastic polyester elastomer typically is used in demanding applications in the automotive, fluid power, electrical/electronic, consumer goods, appliance and power tool, sporting goods, furniture, industrial and off-road transportation/equipment industry.Hytrel® SC988 NC010 is the highest modulus grade, with nominal hardness of 82D, contains a non-discoloring stabilizer. Can be processed by various thermoplastic processing techniques. Developed for applications such as parts for the healthcare industry.SPECIAL CONTROL for HEALTHCARE APPLICATIONSThis product is manufactured according to Good Manufacturing Practice (GMP) principles and generally accepted in food contact applications in the USA when meeting applicable use conditions. This product is also tested against ISO 10993-5 and -11 and selected parts of USP Class VI. For details, individual compliance statements are available from your DuPont representative.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.28 g/cm³

Show Material materials with Density of 1.28 g/cm³

ISO 1183

Water absorption

23.0 °C

0.3 %

Show Material materials with Water absorption of 0.3 %

Sim. to ISO 62 | Immersion 24h

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

1.2 GPa

Show Material materials with Elastic modulus of 1.2 GPa

ISO 527-1/-2

Elongation

23.0 °C

340 %

Show Material materials with Elongation of 340 %

ISO 527-1/-2

Elongation at yield

23.0 °C

19 %

Show Material materials with Elongation at yield of 19 %

ISO 527-1/-2

Flexural modulus

23.0 °C

1.2 GPa

Show Material materials with Flexural modulus of 1.2 GPa

ISO 178

Hardness, Shore D

23.0 °C

76 [-]

Show Material materials with Hardness, Shore D of 76 [-]

max., ISO 7619-1

Impact strength, Charpy notched

-40.0 °C

5 kJ/m²

Show Material materials with Impact strength, Charpy notched of 5 kJ/m²

ISO 179/1eA

-6.0 °C

5 kJ/m²

Show Material materials with Impact strength, Charpy notched of 5 kJ/m²

ISO 179/1eA

23.0 °C

15 kJ/m²

Show Material materials with Impact strength, Charpy notched of 15 kJ/m²

ISO 179/1eA

Impact strength, Izod unnotched

-40.0 °C

5.5 kJ/m²

Show Material materials with Impact strength, Izod unnotched of 5.5 kJ/m²

ISO 180/1A

23.0 °C

11 kJ/m²

Show Material materials with Impact strength, Izod unnotched of 11 kJ/m²

ISO 180/1A

Unlock all property charts

Poisson's ratio

23.0 °C

0.44 [-]

Show Material materials with Poisson's ratio of 0.44 [-]

Tear strength

23.0 °C

228 kN/m

Show Material materials with Tear strength of 228 kN/m

ISO 34-1

Tensile strength

23.0 °C

46 MPa

Show Material materials with Tensile strength of 46 MPa

ISO 527-1/-2

Yield strength

23.0 °C

36 MPa

Show Material materials with Yield strength of 36 MPa

ISO 527-1/-2

Thermal

PropertyTemperatureValueComment

Brittleness temperature

-84 °C

Show Material materials with Brittleness temperature of -84 °C

ISO 974

Coefficient of thermal expansion

23.0 °C

1.5E-4 1/K

Show Material materials with Coefficient of thermal expansion of 1.5E-4 1/K

ISO 11359-1/-2

Coefficient of thermal expansion, transverse

23.0 °C

1.5E-4 1/K

Show Material materials with Coefficient of thermal expansion, transverse of 1.5E-4 1/K

ISO 11359-1/-2

Glass transition temperature

50 °C

Show Material materials with Glass transition temperature of 50 °C

ISO 11357-1/-2 | 18°F/min

Heat deflection temperature, 0.45 MPa

105 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 105 °C

ISO 75-1/-2

Melting point

221 °C

Show Material materials with Melting point of 221 °C

ISO 11357-1/-3 | 18°F/min

Vicat softening temperature

213 °C

Show Material materials with Vicat softening temperature of 213 °C

ISO 306 | 90°F, 2 lbf

Flammability

Burning Behav. at 60mil nom. thickn.: HB class, Thickness tested: 1.5 mm

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

13 g/10min

Show Material materials with Melt mass-flow rate of 13 g/10min

ISO 1133 | 240°C/2.16kg

Melt volume-flow rate

12 cm³/10min

Show Material materials with Melt volume-flow rate of 12 cm³/10min

ISO 1133

Shrinkage

23.0 °C

1.6 %

Show Material materials with Shrinkage of 1.6 %

ISO 294-4, 2577

Shrinkage, transverse

23.0 °C

1.6 %

Show Material materials with Shrinkage, transverse of 1.6 %

ISO 294-4, 2577

Technological properties

Property
Processing methods

Drying Recommended: yes, Drying Temperature: 110°C, Drying Time, Dehumidified Dryer: 2-3h, Processing Moisture Content: ≤0.08%, Melt Temperature Optimum: 250°C, Min. melt temperature: 245°C, Max. melt temperature: 260°C, Mold Temperature Optimum: 45°C, Min. mold temperature: 45°C, Max. mold temperature: 55°C