Hytrel® HTR8241

Alternative and trade names
TPC-ET
Want to keep this datasheet? Save it now in your required format

Description

Hytrel® HTR8241 is a 65 Shore D High Performance Polyester Elastomer Developed for Extrusion

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.24 g/cm³

Show Material materials with Density of 1.24 g/cm³

ISO 1183

Water absorption

23.0 °C

0.7 %

Show Material materials with Water absorption of 0.7 %

Sim. to ISO 62 | 80mil

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

0.36 GPa

Show Material materials with Elastic modulus of 0.36 GPa

ISO 527-1/-2

Elongation

23.0 °C

490 %

Show Material materials with Elongation of 490 %

ISO 527-1/-2

Elongation at yield

23.0 °C

29 %

Show Material materials with Elongation at yield of 29 %

ISO 527-1/-2

Flexural modulus

23.0 °C

0.36 GPa

Show Material materials with Flexural modulus of 0.36 GPa

ISO 178

Hardness, Shore D

23.0 °C

63 [-]

Show Material materials with Hardness, Shore D of 63 [-]

max., ISO 7619-1

Impact strength, Charpy notched

-40.0 °C

10 kJ/m²

Show Material materials with Impact strength, Charpy notched of 10 kJ/m²

No Break @ 23°C, ISO 179/1eU

-6.0 °C

14 kJ/m²

Show Material materials with Impact strength, Charpy notched of 14 kJ/m²

No Break @ 23°C, ISO 179/1eU

Impact strength, Izod unnotched

-40.0 °C

9 kJ/m²

Show Material materials with Impact strength, Izod unnotched of 9 kJ/m²

ISO 180/1A

Poisson's ratio

23.0 °C

0.48 [-]

Show Material materials with Poisson's ratio of 0.48 [-]

Tear strength

23.0 °C

210 kN/m

Show Material materials with Tear strength of 210 kN/m

ISO 34-1

Tear strength, transverse

23.0 °C

200 kN/m

Show Material materials with Tear strength, transverse of 200 kN/m

ISO 34-1

Tensile strength

23.0 °C

45 MPa

Show Material materials with Tensile strength of 45 MPa

ISO 527-1/-2

Yield strength

23.0 °C

22 MPa

Show Material materials with Yield strength of 22 MPa

ISO 527-1/-2

Impact strength, Charpy unnotched

No Break @ 23,-6°C, ISO 179/1eA

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

2E-4 1/K

Show Material materials with Coefficient of thermal expansion of 2E-4 1/K

ISO 11359-1/-2

Coefficient of thermal expansion, transverse

23.0 °C

2E-4 1/K

Show Material materials with Coefficient of thermal expansion, transverse of 2E-4 1/K

ISO 11359-1/-2

Heat deflection temperature, 0.45 MPa

85 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 85 °C

ISO 75-1/-2

Melting point

211 °C

Show Material materials with Melting point of 211 °C

ISO 11357-1/-3 | 18°F/min

Specific heat capacity

23.0 °C

2070 J/(kg·K)

Show Material materials with Specific heat capacity of 2070 J/(kg·K)

of melt

Thermal diffusivity

23.0 °C

0 mm²/s

Show Material materials with Thermal diffusivity of 0 mm²/s

Vicat softening temperature

198 °C

Show Material materials with Vicat softening temperature of 198 °C

ISO 306 | 90°F, 2 lbf

Flammability

FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

600 V

Show Material materials with Comparative tracking index of 600 V

IEC 60112

Dielectric strength

23.0 °C

18 kV/mm

Show Material materials with Dielectric strength of 18 kV/mm

IEC 60243-1

Dissipation factor, 100Hz

23.0 °C

0.01 [-]

Show Material materials with Dissipation factor, 100Hz of 0.01 [-]

IEC 62631-2-1

Dissipation factor, 1MHz

23.0 °C

0.01 [-]

Show Material materials with Dissipation factor, 1MHz of 0.01 [-]

IEC 62631-2-1

Surface resistivity

23.0 °C

2.00E+14 Ω/sq

Show Material materials with Surface resistivity of 2.00E+14 Ω/sq

IEC 62631-3-2

Volume resistivity

23.0 °C

7.00E+12 Ω·cm

Show Material materials with Volume resistivity of 7.00E+12 Ω·cm

IEC 62631-3-1

Rheological Properties

PropertyTemperatureValueComment

Melt volume-flow rate

5 cm³/10min

Show Material materials with Melt volume-flow rate of 5 cm³/10min

ISO 1133

Shrinkage

23.0 °C

1.7 %

Show Material materials with Shrinkage of 1.7 %

ISO 294-4, 2577

Shrinkage, transverse

23.0 °C

1.6 %

Show Material materials with Shrinkage, transverse of 1.6 %

ISO 294-4, 2577

Technological properties

Property
Processing methods

Drying Recommended: yes, Drying Temperature: 110°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.08%, Melt Temperature Optimum: 240°C, Min. melt temperature: 230°C, Max. melt temperature: 250°C, Mold Temperature Optimum: 45°C, Min. mold temperature: 40°C, Max. mold temperature: 50°C