Description

Common features of Hytrel® thermoplastic polyester elastomer include mechanical and physical properties such as exceptional toughness and resilience, high resistance to creep, impact and flex fatigue, flexibility at low temperatures and good retention of properties at elevated temperatures. In addition, it resists many industrial chemicals, oils and solvents. Special grades include heat stabilised, flame retardant, food contact compliant, blow molding and extrusion grades. Concentrates offered include black pigments, UV protection additives, heat stabilisers, and flame retardants. Hytrel® thermoplastic polyester elastomer is plasticiser free.The good melt stability of Hytrel® thermoplastic polyester elastomer normally enables the recycling of properly handled production waste. If recycling is not possible, DuPont recommends, as the preferred option, incineration with energy recovery (-24 kJ/g of base polymer) in appropriately equipped installations.For disposal, local regulations have to be observed. Hytrel® thermoplastic polyester elastomer typically is used in demanding applications in the automotive, fluid power, electrical/electronic, consumer goods, appliance and power tool, sporting goods, furniture, industrial and off-road transportation/equipment industry.Hytrel® PC938 has a very low modulus, nominal hardness of 30D, containing non-discoloring stabilizer. Processed by thermoplastic processing techniques like injection molding and extrusion. Developed for applications such as parts for the healthcare industry.PREMIUM CONTROL for HEALTHCARE APPLICATIONSThis product is manufactured according to Good Manufacturing Practice (GMP) principles and generally accepted in food contact applications in the USA when meeting applicable use conditions. This product is also tested against ISO 10993-5 and -11 and selected parts of USP Class VI and FDA drug and device master files (DMF and MAF) have been established.For details, individual compliance statements are available from your DuPont representative.The below datasheet is a condensed version. For a complete datasheet, please contact your DuPont representative.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.07 g/cm³

Show Material materials with Density of 1.07 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

300 %

Show Material materials with Elongation of 300 %

min. | ISO 527-1/-2

Hardness, Shore D

23.0 °C

30 [-]

Show Material materials with Hardness, Shore D of 30 [-]

max., ISO 7619-1

Tensile strength

23.0 °C

24 MPa

Show Material materials with Tensile strength of 24 MPa

ISO 527-1/-2

Impact strength, Charpy notched

No Break @ 23°C, ISO 179/1eU

Thermal

PropertyValueComment

Melting point

177 °C

Show Material materials with Melting point of 177 °C

ISO 11357-1/-3 | 18°F/min

Flammability

FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min

Technological properties

Property
Processing methods

Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-3h, Processing Moisture Content: ≤0.08%