BS CZ108 (CW508L) Basis Brass

View suppliers (30)
Want to keep this datasheet? Save it now in your required format

Description

2.0321 (CuZn37) basis brass, is one of the most popular grades of brass due to its hot and cold working capabilities. Supplied primarily as a sheet grade, this material is often used for general purpose and simple forming operations. It offers very good corrosion resistance in normal environments and good machinability at slow speeds. It shows the following features and properties:


  • Good hot and cold formability
  • Good combination of strength and ductility
  • Related Standards

    Equivalent Materials

    This material data has been provided by Matmatch.

    "Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    Mechanical

    PropertyTemperatureValue

    Elongation

    23.0 °C

    15 %

    Show Material materials with Elongation of 15 %

    Hardness, Vickers

    23.0 °C

    100 [-]

    Show Material materials with Hardness, Vickers of 100 [-]

    Tensile strength

    23.0 °C

    350 MPa

    Show Material materials with Tensile strength of 350 MPa

    Chemical properties

    PropertyValue

    Copper

    63 %

    Show Material materials with Copper of 63 %

    Zinc

    37 %

    Show Material materials with Zinc of 37 %

    Technological properties

    Property
    Application areas

    Electrical: Lamp caps, lamp-holder and switch components;General: Coppersmithing work for chains, eyelets fasteners, hinges, kicking plates, locks, fingerplates and wire brushes, various cold presswork products including instrument covers and containers, blanked articles such as instrument plates and wheels, cold headed items including pins, rivets and screws, springs, radiator tanks and reflectors

    Cold Forming

    Good cold formability

    Corrosion properties

    Very good corrosion resistance

    General machinability

    Good machinability

    Hot forming

    Very good hot working capabilities.