BS CZ121 (CW614N) Free Machining Brass

View suppliers (29)
Want to keep this datasheet? Save it now in your required format

Description

2.0401 (CuZn39Pb3) is a free-machining brass consisting of a duplex phase structure with a 3% lead content. It is suited to high speed machining operations due its superior machinability, thread rolling and knurling characteristics. Particles of lead are finely dispersed throughout the microstructure, acting as both a lubricant and a chip breaker to give the alloy its free-machining characteristics. 2.0401 (CuZn39Pb3) machinability rating of 100 is the standard against which all copper alloys are rated. It offers good strength, is easily soldered or brazed and has good resistance to corrosion. It shows the following features and properties:


  • Free machining
  • Good corrosion resistance
  • Good strength levels
  • Related Standards

    Equivalent Materials

    This material data has been provided by Matmatch.

    "Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    Mechanical

    PropertyTemperatureValue

    Elongation

    23.0 °C

    15 - 25 %

    Show Material materials with Elongation of 15 - 25 %

    Tensile strength

    23.0 °C

    350 - 425 MPa

    Show Material materials with Tensile strength of 350 - 425 MPa

    Chemical properties

    PropertyValue

    Copper

    58 %

    Show Material materials with Copper of 58 %

    Lead

    3 %

    Show Material materials with Lead of 3 %

    Zinc

    39 %

    Show Material materials with Zinc of 39 %

    Technological properties

    Property
    Application areas

    General: A wide variety of machined components usually made on high speed automatic lathes including nuts, bolts, screws, bushings, bearings, pins and washers, plug pins, switch terminals, lock bodies, hinges, extruded sections, door treads, window frames and trim

    Corrosion properties

    Good corrosion resistance

    General machinability

    Machinability rating: 100%