Mechanical
Property | Temperature | Value |
---|---|---|
Elongation | 23.0 °C | 25 - 40 % Show Material materials with Elongation of 25 - 40 % |
Tensile strength | 23.0 °C | 540 - 590 MPa Show Material materials with Tensile strength of 540 - 590 MPa |
Yield strength | 23.0 °C | 440 - 510 MPa Show Material materials with Yield strength of 440 - 510 MPa |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Decorative trim, marine hardware and sheathing.;Aerospace: Cold workable components.;Other: Architectural panels and decorative trim, coinage, storage tanks, heat exchangers, water boxes, munitions mixing chambers, masonry fixings and non-magnetic instrument casings | |
Cold Forming | Excellent cold working properties | |
Corrosion properties | Excellent corrosion resistance |