General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 7.5 g/cm³ Show Material materials with Density of 7.5 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Charpy impact energy, V-notch | 23.0 °C | 27 J Show Material materials with Charpy impact energy, V-notch of 27 J |
Elongation | 23.0 °C | 17 % Show Material materials with Elongation of 17 % |
Tensile strength | 23.0 °C | 620 - 680 MPa Show Material materials with Tensile strength of 620 - 680 MPa |
Yield strength Rp0.2 | 23.0 °C | 245 - 325 MPa Show Material materials with Yield strength Rp0.2 of 245 - 325 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.8E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.8E-5 1/K | for 0-300°C |
Melting point | 1060 - 1075 °C Show Material materials with Melting point of 1060 - 1075 °C | ||
Thermal conductivity | 23.0 °C | 59 - 67 W/(m·K) Show Material materials with Thermal conductivity of 59 - 67 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 6.96E+6 - 8.12E+6 S/m Show Material materials with Electrical conductivity of 6.96E+6 - 8.12E+6 S/m |
Specific Electrical conductivity | 12 - 14 % IACS Show Material materials with Specific Electrical conductivity of 12 - 14 % IACS |
Magnetic
Property | Temperature | Value |
---|---|---|
Relative magnetic permeability | 23.0 °C | 1.5 [-] Show Material materials with Relative magnetic permeability of 1.5 [-] |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 8.5 - 10 % Show Material materials with Aluminium of 8.5 - 10 % | ||
Copper | Balance | ||
Iron | 4 - 5 % Show Material materials with Iron of 4 - 5 % | ||
Manganese | 0.5 % Show Material materials with Manganese of 0.5 % | max. | |
Nickel | 4.5 - 5.5 % Show Material materials with Nickel of 4.5 - 5.5 % |
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: High performance fasteners, valve and pump components, propeller shafts and weapons handling systems;Other: Pipe fittings, heat exchangers, wear plates, thrust washers, bearings, bushes, safety tools, worm wheels and gears | |
Corrosion properties | Excellent resistance to erosion and corrosion |