COLSPEED 90 Bronze

Want to keep this datasheet? Save it now in your required format

Description

COLSPEED 90 is derived using the basis of a 10/5/5 aluminium bronze with an addition of finely dispersed lead particles with very good self-lubricating and anti-friction properties that improve performance in wear applications. It shows the following features and properties:


  • Very high strength
  • Excellent general corrosion resistance
  • Very high wear and galling resistance
  • Excellent machinability
  • Outstanding bearing properties
  • Spark resistance
  • Retention of properties at cryogenic temperatures
  • Equivalent Materials

    This material data has been provided by Matmatch.

    "Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    Mechanical

    PropertyTemperatureValue

    Elongation

    23.0 °C

    10 - 13 %

    Show Material materials with Elongation of 10 - 13 %

    Hardness, Brinell

    23.0 °C

    200 - 220 [-]

    Show Material materials with Hardness, Brinell of 200 - 220 [-]

    Tensile strength

    23.0 °C

    700 - 760 MPa

    Show Material materials with Tensile strength of 700 - 760 MPa

    Yield strength

    23.0 °C

    400 - 500 MPa

    Show Material materials with Yield strength of 400 - 500 MPa

    Chemical properties

    PropertyValue

    Aluminium

    9.7 %

    Show Material materials with Aluminium of 9.7 %

    Copper

    Balance

    Iron

    3.8 %

    Show Material materials with Iron of 3.8 %

    Lead

    1.75 %

    Show Material materials with Lead of 1.75 %

    Manganese

    1.3 %

    Show Material materials with Manganese of 1.3 %

    Nickel

    5 %

    Show Material materials with Nickel of 5 %

    Technological properties

    Property
    Application areas

    Offshore & marine: Marine hardware, fasteners and fittings;General: Fasteners, gears, non-sparking safety tooling, thrust washers, valve guides, fluid handling equipment, valve spindles and components, bearings pins and bushes, thermostatic valves and worm wheels

    Corrosion properties

    Excellent general corrosion resistance

    General machinability