General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 7.6 g/cm³ Show Material materials with Density of 7.6 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elongation | 23.0 °C | 5 - 12 % Show Material materials with Elongation of 5 - 12 % |
Tensile strength | 23.0 °C | 550 - 760 MPa Show Material materials with Tensile strength of 550 - 760 MPa |
Yield strength Rp0.2 | 23.0 °C | 275 - 415 MPa Show Material materials with Yield strength Rp0.2 of 275 - 415 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.7E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.7E-5 1/K | for 0-300°C |
Melting point | 1050 - 1070 °C Show Material materials with Melting point of 1050 - 1070 °C | ||
Thermal conductivity | 23.0 °C | 38 - 46 W/(m·K) Show Material materials with Thermal conductivity of 38 - 46 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 4.06E+6 - 5.22E+6 S/m Show Material materials with Electrical conductivity of 4.06E+6 - 5.22E+6 S/m |
Specific Electrical conductivity | 7 - 9 % IACS Show Material materials with Specific Electrical conductivity of 7 - 9 % IACS |
Magnetic
Property | Temperature | Value |
---|---|---|
Relative magnetic permeability | 23.0 °C | 1 [-] Show Material materials with Relative magnetic permeability of 1 [-] |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 9 - 11 % Show Material materials with Aluminium of 9 - 11 % | ||
Copper | Balance | ||
Iron | 2 - 4 % Show Material materials with Iron of 2 - 4 % | ||
Manganese | 1.5 % Show Material materials with Manganese of 1.5 % | max. | |
Nickel | 4 - 5.5 % Show Material materials with Nickel of 4 - 5.5 % | ||
Silicon | 0.25 % Show Material materials with Silicon of 0.25 % |
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Marine fasteners, hardware and fittings;Aerospace: Landing gear components, thrust washers, gears, control bushes, faucet balls, springs and worm wheels;Other: Non-sparking safety tooling, valve stems and seats, wear plates, welding clamps, valve spindles and components, fasteners and bearing bushes | |
Corrosion properties | High resistance to corrosion and erosion | |
General machinability | Good machinability | |
Hot forming | Easily hot worked |