Mechanical
Property | Temperature | Value |
---|---|---|
Elongation | 23.0 °C | 12 - 25 % Show Material materials with Elongation of 12 - 25 % |
Tensile strength | 23.0 °C | 280 - 500 MPa Show Material materials with Tensile strength of 280 - 500 MPa |
Yield strength Rp0.2 | 23.0 °C | 380 - 420 MPa Show Material materials with Yield strength Rp0.2 of 380 - 420 MPa |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Marine hardware and fasteners;Power generation: Electrical springs and contacts;Other: Pump and valve spindles, fasteners, sleeve bushings, springs, shafts, flanges, architectural and decorative components, lock washers, spring washers and masonry fixings | |
Cold Forming | Good cold formability | |
Corrosion properties | Very good corrosion resistance | |
General machinability | Machinability Rating: 20 |