General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 8.53 g/cm³ Show Material materials with Density of 8.53 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Charpy impact energy, V-notch | 23.0 °C | 40 J Show Material materials with Charpy impact energy, V-notch of 40 J |
Elongation | 23.0 °C | 18 - 22 % Show Material materials with Elongation of 18 - 22 % |
Tensile strength | 23.0 °C | 710 - 725 MPa Show Material materials with Tensile strength of 710 - 725 MPa |
Yield strength Rp0.2 | 23.0 °C | 400 - 430 MPa Show Material materials with Yield strength Rp0.2 of 400 - 430 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.6E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.6E-5 1/K | for 0-400°C |
Melting point | 1030 - 1085 °C Show Material materials with Melting point of 1030 - 1085 °C | ||
Thermal conductivity | 23.0 °C | 25 W/(m·K) Show Material materials with Thermal conductivity of 25 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical resistivity | 23.0 °C | 3.5E-7 Ω·m Show Material materials with Electrical resistivity of 3.5E-7 Ω·m |
Magnetic
Property | Temperature | Value | Comment |
---|---|---|---|
Relative magnetic permeability | 23.0 °C | 1.01 [-] Show Material materials with Relative magnetic permeability of 1.01 [-] | max. |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 1 - 2 % Show Material materials with Aluminium of 1 - 2 % | ||
Chromium | 0.5 % Show Material materials with Chromium of 0.5 % | ||
Copper | Balance | ||
Iron | 0.7 - 1.2 % Show Material materials with Iron of 0.7 - 1.2 % | ||
Manganese | 3.5 - 5.5 % Show Material materials with Manganese of 3.5 - 5.5 % | ||
Nickel | 13.5 - 16.5 % Show Material materials with Nickel of 13.5 - 16.5 % | ||
Other | 0.3 % Show Material materials with Other of 0.3 % | max., Inosinic acid (IMP) |
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Critical marine fasteners, gears, shafts, pipe couplings, sonar equipment, connectors, flanges and subsea components | |
Corrosion properties | Excellent corrosion and pitting resistance in marine environments | |
General machinability | Easily machined |