General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 8.87 g/cm³ Show Material materials with Density of 8.87 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 150 GPa Show Material materials with Elastic modulus of 150 GPa |
Elongation | 23.0 °C | 18 % Show Material materials with Elongation of 18 % |
Hardness, Vickers | 23.0 °C | 159 - 207 [-] Show Material materials with Hardness, Vickers of 159 - 207 [-] |
Shear modulus | 23.0 °C | 106 GPa Show Material materials with Shear modulus of 106 GPa |
Tensile strength | 23.0 °C | 580 MPa Show Material materials with Tensile strength of 580 MPa |
Yield strength Rp0.2 | 23.0 °C | 430 MPa Show Material materials with Yield strength Rp0.2 of 430 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Specific heat capacity | 23.0 °C | 419 J/(kg·K) Show Material materials with Specific heat capacity of 419 J/(kg·K) |
Thermal conductivity | 23.0 °C | 190 W/(m·K) Show Material materials with Thermal conductivity of 190 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical resistivity | 23.0 °C | 2.5E-7 Ω·m Show Material materials with Electrical resistivity of 2.5E-7 Ω·m |
Specific Electrical conductivity | 6.9 % IACS Show Material materials with Specific Electrical conductivity of 6.9 % IACS |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Offshore & marine: Non-magnetic naval architecture and high strength fasteners (non-magnetic and cryogenic);Aerospace: Bearing cages, aircraft undercarriage components, fasteners and bearings;Other: Fasteners, engine valve guides and seats, pump and valve components, high performance bearings, bushes, gears safety tools, mechanical seals, electrical contacts, resistance welding electrodes and brake pads | |
Corrosion properties | Excellent corrosion resistance |