TROJAN Copper Alloy

Want to keep this datasheet? Save it now in your required format

Description

2.0857 (CuNi3Si) ultimate super strength copper nickel silicon alloy, specially developed to provide a unique blend of mechnical and physical properties for high performance engineering. It has similar characteristics to Colsibro®, although Trojan is produced with increased levels of nickel and silicon in order to further increase the mechanical strength. It shows the following features and properties:


  • Ultra-high strength
  • High electrical and thermal conductivity
  • Excellent wear and galling resistance
  • Extremely low magnetic permeability
  • Excellent general corrosion resistance
  • Outstanding bearing properties
  • Spark resistance
  • Good machinability and dimensional stability
  • Outstanding low temperature mechanical properties
  • Related Standards

    Equivalent Materials

    This material data has been provided by Matmatch.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyTemperatureValue

    Density

    23.0 °C

    8.8 g/cm³

    Show Material materials with Density of 8.8 g/cm³

    Mechanical

    PropertyTemperatureValue

    Elongation

    23.0 °C

    10 %

    Show Material materials with Elongation of 10 %

    Hardness, Brinell

    23.0 °C

    190 - 200 [-]

    Show Material materials with Hardness, Brinell of 190 - 200 [-]

    Tensile strength

    23.0 °C

    690 - 800 MPa

    Show Material materials with Tensile strength of 690 - 800 MPa

    Yield strength Rp0.2

    23.0 °C

    570 - 750 MPa

    Show Material materials with Yield strength Rp0.2 of 570 - 750 MPa

    Thermal

    PropertyTemperatureValueComment

    Coefficient of thermal expansion

    23.0 °C

    1.6E-5 1/K

    Show Material materials with Coefficient of thermal expansion of 1.6E-5 1/K

    for 0-400°C

    Melting point

    1060 - 1085 °C

    Show Material materials with Melting point of 1060 - 1085 °C

    Thermal conductivity

    23.0 °C

    159 W/(m·K)

    Show Material materials with Thermal conductivity of 159 W/(m·K)

    Electrical

    PropertyTemperatureValue

    Electrical conductivity

    23.0 °C

    1.74E+7 S/m

    Show Material materials with Electrical conductivity of 1.74E+7 S/m

    Specific Electrical conductivity

    30 % IACS

    Show Material materials with Specific Electrical conductivity of 30 % IACS

    Magnetic

    PropertyTemperatureValue

    Relative magnetic permeability

    23.0 °C

    1 [-]

    Show Material materials with Relative magnetic permeability of 1 [-]

    Chemical properties

    PropertyValue

    Copper

    Balance

    Nickel

    2.6 - 4.5 %

    Show Material materials with Nickel of 2.6 - 4.5 %

    Silicon

    0.8 - 1.3 %

    Show Material materials with Silicon of 0.8 - 1.3 %

    Technological properties

    Property
    Application areas

    Automotive: valve guides, bushes and valve seats;Electrical: current-carrying electrical components such as slip rings, squirrel cages, springs, rotary switch contacts, contact blades, short-circuit rings and heavy duty switchgear;Offshore & marine: Downhole tools, shear pins, hydraulic valve bodies, pump components and ball valves and mechanical seals;Other: Non-magnetic tooling, plastic mould tooling, friction pads and fibre optic connectors

    Corrosion properties

    Excellent corrosion resistance

    General machinability

    Good machinability