Beryllium Copper (BECOL-25) TH04

View suppliers (16)
Want to keep this datasheet? Save it now in your required format

Description

C17510 TH04, contains around 2% nickel and features good mechanical properties, high electrical conductivity and very good machinability. As a result, it has moderate strength and finds application in current-carrying springs, thermal control devices, welding electrodes and power connectors.

Related Standards

Equivalent Materials

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.75 g/cm³

Show Material materials with Density of 8.75 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

132 GPa

Show Material materials with Elastic modulus of 132 GPa

Elongation

23.0 °C

5 %

Show Material materials with Elongation of 5 %

Hardness, Rockwell C

23.0 °C

18 - 26 [-]

Show Material materials with Hardness, Rockwell C of 18 - 26 [-]

Shear modulus

23.0 °C

52 GPa

Show Material materials with Shear modulus of 52 GPa

Tensile strength

23.0 °C

750 - 950 MPa

Show Material materials with Tensile strength of 750 - 950 MPa

Yield strength Rp0.2

23.0 °C

670 - 900 MPa

Show Material materials with Yield strength Rp0.2 of 670 - 900 MPa

Thermal

PropertyTemperatureValue

Thermal conductivity

23.0 °C

167 - 260 W/(m·K)

Show Material materials with Thermal conductivity of 167 - 260 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

3.8E-8 Ω·m

Show Material materials with Electrical resistivity of 3.8E-8 Ω·m

Specific Electrical conductivity

50 % IACS

Show Material materials with Specific Electrical conductivity of 50 % IACS

Chemical properties

PropertyValue

Beryllium

0.2 - 0.6 %

Show Material materials with Beryllium of 0.2 - 0.6 %

Copper

Balance

Nickel

1.8 - 2.2 %

Show Material materials with Nickel of 1.8 - 2.2 %

Technological properties

Property
Application areas

Aerospace: Landing gear, bearing bushes and high performance fasteners;Automotive: Valve guides, bushes and valve seats;Offshore & marine: Offshore drilling and instrumentation equipment, downhole tooling, valve, pump and shaft components;Other: Deep drawing tooling, plastic moulding dies, tools and plungers, die-casting plunger tips, non-magnetic and non sparking tools, electrical and electronic connectors, springs, fasteners, switchgear, resistance welding electrodes and equipment, flash butt welding dies and inserts, seam welding electrode shafts

Corrosion properties

High corrosion resistance

General machinability

Very good machinability