BS NS101 Nickel Silver

View suppliers (1)
Want to keep this datasheet? Save it now in your required format

Description

NS101 (CuNi10Zn42Pb2) is the general purpose grade of nickel silver most commonly used for hot stamping to complex shapes and as machining rod for a wide variety of electrical and electronic components. It has good corrosion and tarnish resistance and is frequently specified for many architectural applications where best use is made of its pleasing silvery gold colour and resistance to atmospheric corrosion.

Equivalent Materials

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.47 g/cm³

Show Material materials with Density of 8.47 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

100 GPa

Show Material materials with Elastic modulus of 100 GPa

Elongation

23.0 °C

20 %

Show Material materials with Elongation of 20 %

Hardness, Vickers

23.0 °C

130 [-]

Show Material materials with Hardness, Vickers of 130 [-]

Tensile strength

23.0 °C

520 MPa

Show Material materials with Tensile strength of 520 MPa

Yield strength Rp0.2

23.0 °C

230 MPa

Show Material materials with Yield strength Rp0.2 of 230 MPa

Thermal

PropertyTemperatureValue

Melting point

940 - 980 °C

Show Material materials with Melting point of 940 - 980 °C

Thermal conductivity

23.0 °C

46 W/(m·K)

Show Material materials with Thermal conductivity of 46 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

5.22E+6 S/m

Show Material materials with Electrical conductivity of 5.22E+6 S/m

Electrical resistivity

23.0 °C

1.8E-7 Ω·m

Show Material materials with Electrical resistivity of 1.8E-7 Ω·m

Specific Electrical conductivity

9 % IACS

Show Material materials with Specific Electrical conductivity of 9 % IACS

Magnetic

PropertyTemperatureValueComment

Relative magnetic permeability

23.0 °C

1.05 [-]

Show Material materials with Relative magnetic permeability of 1.05 [-]

max.

Chemical properties

PropertyValueComment

Copper

44 - 47 %

Show Material materials with Copper of 44 - 47 %

Iron

0.4 %

Show Material materials with Iron of 0.4 %

max.

Lead

1 - 2.5 %

Show Material materials with Lead of 1 - 2.5 %

Manganese

0.2 - 0.5 %

Show Material materials with Manganese of 0.2 - 0.5 %

Nickel

9 - 11 %

Show Material materials with Nickel of 9 - 11 %

Zinc

Balance

Technological properties

Property
Application areas

Frequently used applications of NS101 include gears, pinions, clock and watch parts, screws and other types of fasteners, hot stampings and forgings, keys, lock parts, door furniture, grills, decorative and architectural metalwork, darts, fishing tackle, camera, binocular and microscope parts, musical instrument valves and fittings, electrical and electronic pins and connectors and switchgear components.

Corrosion properties

Good corrosion resistance

General machinability

Very good machining and hot stamping characteristics

Looking for suppliers of this material? Click to see 1 supplier of BS NS101 Nickel Silver on Matmatch