General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 8.44 g/cm³ Show Material materials with Density of 8.44 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 120 GPa Show Material materials with Elastic modulus of 120 GPa |
Elongation | 23.0 °C | 20 % Show Material materials with Elongation of 20 % |
Hardness, Vickers | 23.0 °C | 185 [-] Show Material materials with Hardness, Vickers of 185 [-] |
Tensile strength | 23.0 °C | 560 MPa Show Material materials with Tensile strength of 560 MPa |
Yield strength Rp0.2 | 23.0 °C | 450 MPa Show Material materials with Yield strength Rp0.2 of 450 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Melting point | 850 - 870 °C Show Material materials with Melting point of 850 - 870 °C | |
Thermal conductivity | 23.0 °C | 30 W/(m·K) Show Material materials with Thermal conductivity of 30 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 2.90E+6 S/m Show Material materials with Electrical conductivity of 2.90E+6 S/m |
Electrical resistivity | 23.0 °C | 3.4E-7 Ω·m Show Material materials with Electrical resistivity of 3.4E-7 Ω·m |
Specific Electrical conductivity | 5 % IACS Show Material materials with Specific Electrical conductivity of 5 % IACS |
Magnetic
Property | Temperature | Value | Comment |
---|---|---|---|
Relative magnetic permeability | 23.0 °C | 1.05 [-] Show Material materials with Relative magnetic permeability of 1.05 [-] | max. |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Copper | 47 - 50 % Show Material materials with Copper of 47 - 50 % | ||
Iron | 0.3 % Show Material materials with Iron of 0.3 % | max. | |
Lead | 2.3 - 3.3 % Show Material materials with Lead of 2.3 - 3.3 % | ||
Manganese | 1.5 - 3 % Show Material materials with Manganese of 1.5 - 3 % | ||
Nickel | 6 - 8 % Show Material materials with Nickel of 6 - 8 % | ||
Zinc | Balance |
Technological properties
Property | ||
---|---|---|
Application areas | General: Gears, pinions, clock and watch parts, screws and fasteners, keys, lock parts, decorative and architectural metalwork, camera parts, electrical and electronic pins and connectors, medical, industrial and scientific instrument components | |
Corrosion properties | Very high corrosion resistance | |
General machinability | Excellent machinability |