Constantan® Resistance Alloy Foil

Want to keep this datasheet? Save it now in your required format

Description

Constantan is a copper-nickel alloy. It is manufactured under close control from electrolytic copper and pure nickel, and it is available in the form of a foil.

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.9 g/cm³

Show Material materials with Density of 8.9 g/cm³

Mechanical

PropertyTemperatureValueComment

Tensile strength

23.0 °C

480 MPa

Show Material materials with Tensile strength of 480 MPa

annealed

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

200.0 °C

1.45E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.45E-5 1/K

Melting point

1225 - 1300 °C

Show Material materials with Melting point of 1225 - 1300 °C

Specific heat capacity

23.0 °C

395 J/(kg·K)

Show Material materials with Specific heat capacity of 395 J/(kg·K)

Thermal conductivity

100.0 °C

25.3 W/(m·K)

Show Material materials with Thermal conductivity of 25.3 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

5.2E-7 Ω·m

Show Material materials with Electrical resistivity of 5.2E-7 Ω·m

Temperature coefficient of resistance

23.0 °C

2E-5 1/K

Show Material materials with Temperature coefficient of resistance of 2E-5 1/K

Chemical properties

PropertyValue

Chromium

45 %

Show Material materials with Chromium of 45 %

Copper

55 %

Show Material materials with Copper of 55 %

Technological properties

Property
Application areas

It is an ideal alloy for winding heavy-duty industrial rheostats and electric motor starter resistances. High specific resistance, together with good ductility and resistance to corrosion are all-important requirements in the category, and Constantans satisfies the most demanding specifications. It is commonly used as a thermocouple alloy, in conjunctions with copper up to 400 °C and with iron up to 800 °C. In addition, it is used in precision resistors, temperature stable potentiometer, volume control devices and strain gauges. In the resistor field, its high resistance and negligible temperature coefficient of resistance are its main attractions.