General
Property | Value | Shape | Related Standards |
---|---|---|---|
Density | 4.54 g/cm³ Show Material materials with Density of 4.54 g/cm³ | Sheet, Plate, Billet | |
4.54 g/cm³ Show Material materials with Density of 4.54 g/cm³ | Billet | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 |
Dimension
Property | Value | Shape |
---|---|---|
Diameter | 130 mm Show Material materials with Diameter of 130 mm | Billet |
350 mm Show Material materials with Diameter of 350 mm | Billet | |
Length | 1500 mm Show Material materials with Length of 1500 mm | Sheet, Plate |
3000 mm Show Material materials with Length of 3000 mm | Billet | |
4500 mm Show Material materials with Length of 4500 mm | Billet | |
5000 mm Show Material materials with Length of 5000 mm | Sheet | |
6500 mm Show Material materials with Length of 6500 mm | Plate | |
Width | 400 mm Show Material materials with Width of 400 mm | Sheet |
600 mm Show Material materials with Width of 600 mm | Plate | |
1524 mm Show Material materials with Width of 1524 mm | Sheet | |
1600 mm Show Material materials with Width of 1600 mm | Plate |
valueMetaData
Property | Value |
---|
Mechanical
Property | Value | Related Standards | Shape |
---|---|---|---|
Elastic modulus | 114 GPa Show Material materials with Elastic modulus of 114 GPa | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet |
117.0 GPa Show Material materials with Elastic modulus of 117.0 GPa | Sheet, Plate, Billet | ||
Elongation | 10.0 % Show Material materials with Elongation of 10.0 % | Sheet, Plate, Billet | |
Hardness, Brinell | 411.0 Show Material materials with Hardness, Brinell of 411.0 | Sheet, Plate, Billet | |
Hardness, Rockwell C | 44.0 [-] Show Material materials with Hardness, Rockwell C of 44.0 [-] | Sheet, Plate, Billet | |
Hardness, Vickers | 430.0 Show Material materials with Hardness, Vickers of 430.0 | Sheet, Plate, Billet | |
Impact strength, Charpy notched | 16.0 - 19.0 kJ/m² Show Material materials with Impact strength, Charpy notched of 16.0 - 19.0 kJ/m² | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet |
Poisson's ratio | 0.32 [-] Show Material materials with Poisson's ratio of 0.32 [-] | Sheet, Plate, Billet | |
Shear modulus | 45.0 GPa Show Material materials with Shear modulus of 45.0 GPa | Sheet, Plate, Billet | |
Tensile strength | 1034.0 MPa Show Material materials with Tensile strength of 1034.0 MPa | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet |
1280.0 MPa Show Material materials with Tensile strength of 1280.0 MPa | Sheet, Plate, Billet | ||
Yield strength | 965.0 MPa Show Material materials with Yield strength of 965.0 MPa | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet |
1210.0 MPa Show Material materials with Yield strength of 1210.0 MPa | Sheet, Plate, Billet |
Thermal
Property | Temperature | Value | Related Standards | Shape |
---|---|---|---|---|
Coefficient of thermal expansion | 20 °C | 0.000009 1/K Show Material materials with Coefficient of thermal expansion of 0.000009 1/K | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet |
20 °C | 0.0000093 1/K Show Material materials with Coefficient of thermal expansion of 0.0000093 1/K | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet | |
20 °C | 0.0000095 1/K Show Material materials with Coefficient of thermal expansion of 0.0000095 1/K | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet | |
100 °C | 0.000009 1/K Show Material materials with Coefficient of thermal expansion of 0.000009 1/K | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet | |
315 °C | 0.0000093 1/K Show Material materials with Coefficient of thermal expansion of 0.0000093 1/K | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet | |
538 °C | 0.0000095 1/K Show Material materials with Coefficient of thermal expansion of 0.0000095 1/K | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet | |
Melting point | 1627.0 - 1649.0 °C Show Material materials with Melting point of 1627.0 - 1649.0 °C | Sheet, Plate, Billet | ||
1650.0 °C Show Material materials with Melting point of 1650.0 °C | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet | ||
Specific heat capacity | 635 J/(kg·K) Show Material materials with Specific heat capacity of 635 J/(kg·K) | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet | |
Thermal conductivity | 5.5 W/(m·K) Show Material materials with Thermal conductivity of 5.5 W/(m·K) | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet | |
6.6 W/(m·K) Show Material materials with Thermal conductivity of 6.6 W/(m·K) | Sheet, Plate, Billet |
Electrical
Property | Value | Related Standards | Shape |
---|---|---|---|
Electrical resistivity | 1.57e-06 Ω·m Show Material materials with Electrical resistivity of 1.57e-06 Ω·m | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminium | 5.0 - 6.0 % Show Material materials with Aluminium of 5.0 - 6.0 % | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Sheet, Plate, Billet |
Carbon | 0.05 Show Material materials with Carbon of 0.05 | Sheet, Plate, Billet | |
0.08 Show Material materials with Carbon of 0.08 | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet | |
Copper | 0.35 - 1.0 % Show Material materials with Copper of 0.35 - 1.0 % | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet |
Hydrogen | 0.0125 Show Material materials with Hydrogen of 0.0125 | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Billet |
0.015 Show Material materials with Hydrogen of 0.015 | Sheet, Plate, Billet | ||
Iron | 0.35 - 1.0 % Show Material materials with Iron of 0.35 - 1.0 % | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Sheet, Plate, Billet |
Nitrogen | 0.04 Show Material materials with Nitrogen of 0.04 | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Sheet, Plate, Billet |
Oxygen | 0.2 Show Material materials with Oxygen of 0.2 | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Sheet, Plate, Billet |
Tin | 1.5 - 2.5 % Show Material materials with Tin of 1.5 - 2.5 % | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Sheet, Plate, Billet |
Vanadium | 5.0 - 6.0 % Show Material materials with Vanadium of 5.0 - 6.0 % | AMS 4918, AMS 4936, AMS 4971, AMS 4978, AMS 4979, MIL-T 9046, MIL-T 9047 | Sheet, Plate, Billet |