This alloy UNS R56410 is a Titanium Beta Alloy. It is harder and stronger than many titanium alloys. This Titanium is a heat treatable alloy, it’s weldable and it’s easily formed. The chief problems for this alloy include flank wear, spring-back and chip control. Because of these characteristics, positive rake chip grooves in combination with light hones on the cutting edge are advantageous.

Equivalent Materials

This material data has been provided by VSMPO,Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueShape

Density

4.65 g/cm³

Show Material materials with Density of 4.65 g/cm³

Bar, Billet

Dimension

PropertyTemperatureValueShapeComment

Diameter

7 mm

Show Material materials with Diameter of 7 mm

Bar

115 mm

Show Material materials with Diameter of 115 mm

Bar

130 mm

Show Material materials with Diameter of 130 mm

Billet

350 mm

Show Material materials with Diameter of 350 mm

Billet

Dimensions

15-65 mm diameter up to 6000 mm length °C

7-14.5 mm diameter up to 3000 mm length

Bar

Length

3000 mm

Show Material materials with Length of 3000 mm

Billet

4500 mm

Show Material materials with Length of 4500 mm

Billet

6000 mm

Show Material materials with Length of 6000 mm

Bar

max

Mechanical

PropertyValueShape

Elastic modulus

110.0

Show Material materials with Elastic modulus of 110.0

Bar, Billet

Elongation

9.0 %

Show Material materials with Elongation of 9.0 %

Bar, Billet

Hardness, Brinell

304.0

Show Material materials with Hardness, Brinell of 304.0

Bar, Billet

Hardness, Rockwell C

32.0 [-]

Show Material materials with Hardness, Rockwell C of 32.0 [-]

Bar, Billet

Hardness, Vickers

318.0

Show Material materials with Hardness, Vickers of 318.0

Bar, Billet

Shear modulus

41.0 GPa

Show Material materials with Shear modulus of 41.0 GPa

Bar, Billet

Tensile strength

970.0 MPa

Show Material materials with Tensile strength of 970.0 MPa

Bar, Billet

Yield strength

900.0 MPa

Show Material materials with Yield strength of 900.0 MPa

Bar, Billet

Thermal

PropertyValueShapeComment

Coefficient of thermal expansion

7.099999999999997e-06 - 9.699999999999999e-06 1/K

Show Material materials with Coefficient of thermal expansion of 7.099999999999997e-06 - 9.699999999999999e-06 1/K

Typical for Titanium Beta Alloy

Melting point

1550.0 - 1815.0 °C

Show Material materials with Melting point of 1550.0 - 1815.0 °C

Typical for Titanium Beta Alloy

Specific heat capacity

490.0 - 580.0 J/(kg·K)

Show Material materials with Specific heat capacity of 490.0 - 580.0 J/(kg·K)

Typical for Titanium Beta Alloy

Thermal conductivity

7.8 W/(m·K)

Show Material materials with Thermal conductivity of 7.8 W/(m·K)

Bar, Billet

Chemical properties

PropertyValueShape

Aluminium

2.6 - 3.4 %

Show Material materials with Aluminium of 2.6 - 3.4 %

Bar, Billet

Carbon

0.05 %

Show Material materials with Carbon of 0.05 %

Bar, Billet

Hydrogen

0.015

Show Material materials with Hydrogen of 0.015

Bar, Billet

Iron

1.6 - 2.2 %

Show Material materials with Iron of 1.6 - 2.2 %

Bar, Billet

Nitrogen

0.05

Show Material materials with Nitrogen of 0.05

Bar, Billet

Oxygen

0.13

Show Material materials with Oxygen of 0.13

Bar, Billet

Vanadium

9.0 - 11.0 %

Show Material materials with Vanadium of 9.0 - 11.0 %

Bar, Billet