General
Property | Value | Shape |
---|---|---|
Density | 4.65 g/cm³ Show Material materials with Density of 4.65 g/cm³ | Bar, Billet |
Dimension
Property | Temperature | Value | Shape | Comment |
---|---|---|---|---|
Diameter | 7 mm Show Material materials with Diameter of 7 mm | Bar | ||
115 mm Show Material materials with Diameter of 115 mm | Bar | |||
130 mm Show Material materials with Diameter of 130 mm | Billet | |||
350 mm Show Material materials with Diameter of 350 mm | Billet | |||
Dimensions | 15-65 mm diameter up to 6000 mm length °C | 7-14.5 mm diameter up to 3000 mm length | Bar | |
Length | 3000 mm Show Material materials with Length of 3000 mm | Billet | ||
4500 mm Show Material materials with Length of 4500 mm | Billet | |||
6000 mm Show Material materials with Length of 6000 mm | Bar | max |
Mechanical
Property | Value | Shape |
---|---|---|
Elastic modulus | 110.0 Show Material materials with Elastic modulus of 110.0 | Bar, Billet |
Elongation | 9.0 % Show Material materials with Elongation of 9.0 % | Bar, Billet |
Hardness, Brinell | 304.0 Show Material materials with Hardness, Brinell of 304.0 | Bar, Billet |
Hardness, Rockwell C | 32.0 [-] Show Material materials with Hardness, Rockwell C of 32.0 [-] | Bar, Billet |
Hardness, Vickers | 318.0 Show Material materials with Hardness, Vickers of 318.0 | Bar, Billet |
Shear modulus | 41.0 GPa Show Material materials with Shear modulus of 41.0 GPa | Bar, Billet |
Tensile strength | 970.0 MPa Show Material materials with Tensile strength of 970.0 MPa | Bar, Billet |
Yield strength | 900.0 MPa Show Material materials with Yield strength of 900.0 MPa | Bar, Billet |
Thermal
Property | Value | Shape | Comment |
---|---|---|---|
Coefficient of thermal expansion | 7.099999999999997e-06 - 9.699999999999999e-06 1/K Show Material materials with Coefficient of thermal expansion of 7.099999999999997e-06 - 9.699999999999999e-06 1/K | Typical for Titanium Beta Alloy | |
Melting point | 1550.0 - 1815.0 °C Show Material materials with Melting point of 1550.0 - 1815.0 °C | Typical for Titanium Beta Alloy | |
Specific heat capacity | 490.0 - 580.0 J/(kg·K) Show Material materials with Specific heat capacity of 490.0 - 580.0 J/(kg·K) | Typical for Titanium Beta Alloy | |
Thermal conductivity | 7.8 W/(m·K) Show Material materials with Thermal conductivity of 7.8 W/(m·K) | Bar, Billet |
Chemical properties
Property | Value | Shape |
---|---|---|
Aluminium | 2.6 - 3.4 % Show Material materials with Aluminium of 2.6 - 3.4 % | Bar, Billet |
Carbon | 0.05 % Show Material materials with Carbon of 0.05 % | Bar, Billet |
Hydrogen | 0.015 Show Material materials with Hydrogen of 0.015 | Bar, Billet |
Iron | 1.6 - 2.2 % Show Material materials with Iron of 1.6 - 2.2 % | Bar, Billet |
Nitrogen | 0.05 Show Material materials with Nitrogen of 0.05 | Bar, Billet |
Oxygen | 0.13 Show Material materials with Oxygen of 0.13 | Bar, Billet |
Vanadium | 9.0 - 11.0 % Show Material materials with Vanadium of 9.0 - 11.0 % | Bar, Billet |