General
Property | Value | Related Standards | Shape |
---|---|---|---|
Density | 4.54 g/cm³ Show Material materials with Density of 4.54 g/cm³ | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Bar, Billet |
4.54 g/cm³ Show Material materials with Density of 4.54 g/cm³ | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 |
Dimension
Property | Temperature | Value | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Diameter | 7 mm Show Material materials with Diameter of 7 mm | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142 | Bar | ||
115 mm Show Material materials with Diameter of 115 mm | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142 | Bar | |||
130 mm Show Material materials with Diameter of 130 mm | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556, MIL-F-82142 | Billet | |||
350 mm Show Material materials with Diameter of 350 mm | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556, MIL-F-82142 | Billet | |||
Dimensions | 15-65 mm diameter up to 6000 mm length °C | 7-14.5 mm diameter up to 3000 mm length | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142 | Bar | |
Length | 3000 mm Show Material materials with Length of 3000 mm | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556, MIL-F-82142 | Billet | ||
4500 mm Show Material materials with Length of 4500 mm | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556, MIL-F-82142 | Billet | |||
6000 mm Show Material materials with Length of 6000 mm | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142 | Bar | max |
Mechanical
Property | Value | Related Standards | Shape |
---|---|---|---|
Elastic modulus | 114 GPa Show Material materials with Elastic modulus of 114 GPa | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 | |
118.0 GPa Show Material materials with Elastic modulus of 118.0 GPa | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Bar, Billet | |
Elongation | 13.0 % Show Material materials with Elongation of 13.0 % | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Bar, Billet |
Hardness, Brinell | 318.0 Show Material materials with Hardness, Brinell of 318.0 | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Bar, Billet |
Hardness, Rockwell C | 34.0 Show Material materials with Hardness, Rockwell C of 34.0 | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Bar, Billet |
Hardness, Vickers | 333.0 Show Material materials with Hardness, Vickers of 333.0 | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Bar, Billet |
Poisson's ratio | 0.325 [-] Show Material materials with Poisson's ratio of 0.325 [-] | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Bar, Billet |
Shear modulus | 44.5 GPa Show Material materials with Shear modulus of 44.5 GPa | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Bar, Billet |
Tensile strength | 996.0 MPa Show Material materials with Tensile strength of 996.0 MPa | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 | |
1110.0 MPa Show Material materials with Tensile strength of 1110.0 MPa | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Bar, Billet | |
Yield strength | 827.0 MPa Show Material materials with Yield strength of 827.0 MPa | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 | |
1050.0 MPa Show Material materials with Yield strength of 1050.0 MPa | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Bar, Billet |
Thermal
Property | Temperature | Value | Related Standards | Shape |
---|---|---|---|---|
Coefficient of thermal expansion | 20 °C | 0.0000077 1/K Show Material materials with Coefficient of thermal expansion of 0.0000077 1/K | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 | |
Melting point | 1704.0 °C Show Material materials with Melting point of 1704.0 °C | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 | ||
1705.0 °C Show Material materials with Melting point of 1705.0 °C | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Bar, Billet | ||
Specific heat capacity | 460 J/(kg·K) Show Material materials with Specific heat capacity of 460 J/(kg·K) | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 | ||
Thermal conductivity | 7 W/(m·K) Show Material materials with Thermal conductivity of 7 W/(m·K) | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Bar, Billet | |
7.7 W/(m·K) Show Material materials with Thermal conductivity of 7.7 W/(m·K) | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 |
Electrical
Property | Value | Related Standards |
---|---|---|
Electrical resistivity | 1.85e-06 Ω·m Show Material materials with Electrical resistivity of 1.85e-06 Ω·m | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminium | 5.5 - 6.5 % Show Material materials with Aluminium of 5.5 - 6.5 % | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142, AMS 4975, AMS 4919 | Bar, Billet |
Carbon | 0.05 Show Material materials with Carbon of 0.05 | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Bar, Billet |
0.08 Show Material materials with Carbon of 0.08 | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 | ||
Hydrogen | 0.01 Show Material materials with Hydrogen of 0.01 | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 | |
0.015 Show Material materials with Hydrogen of 0.015 | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Bar, Billet | |
Iron | 0.25 Show Material materials with Iron of 0.25 | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142, AMS 4975, AMS 4919 | Bar, Billet |
Molybdenum | 1.75 - 2.25 % Show Material materials with Molybdenum of 1.75 - 2.25 % | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 | |
1.8 - 2.2 % Show Material materials with Molybdenum of 1.8 - 2.2 % | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Bar, Billet | |
Nitrogen | 0.05 Show Material materials with Nitrogen of 0.05 | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142, AMS 4975, AMS 4919 | Bar, Billet |
Oxygen | 0.12 Show Material materials with Oxygen of 0.12 | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142, AMS 4975, AMS 4919 | Bar, Billet |
Silicon | 0.06 - 0.1 % Show Material materials with Silicon of 0.06 - 0.1 % | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Bar, Billet |
0.1 % Show Material materials with Silicon of 0.1 % | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 | ||
Tin | 1.75 - 2.25 % Show Material materials with Tin of 1.75 - 2.25 % | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 | |
1.8 - 2.2 % Show Material materials with Tin of 1.8 - 2.2 % | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Bar, Billet | |
Zirconium | 3.5 - 4.5 % Show Material materials with Zirconium of 3.5 - 4.5 % | AMS 4975, AMS 4976, AMS 4919, MIL-T 9046, MIL-T 9047 | |
3.6 - 4.4 % Show Material materials with Zirconium of 3.6 - 4.4 % | AMS 4919, AMS 4975, AMS 4976, AMS 4979, AMS T 9047, MIL-T 9046, MIL-T 9047, MIL-F-81556 MIL-F-82142, MIL-F-81556, MIL-F-82142 | Bar, Billet |