Description

This reference material is available in clad products.

Equivalent Materials

This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.78 g/cm³

Show Material materials with Density of 8.78 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

123 GPa

Show Material materials with Elastic modulus of 123 GPa

Tensile strength

23.0 °C

345 MPa

Show Material materials with Tensile strength of 345 MPa

Yield strength

23.0 °C

220 MPa

Show Material materials with Yield strength of 220 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.54E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.54E-5 1/K

Specific heat capacity

23.0 °C

380 J/(kg·K)

Show Material materials with Specific heat capacity of 380 J/(kg·K)

Thermal conductivity

23.0 °C

262 W/(m·K)

Show Material materials with Thermal conductivity of 262 W/(m·K)