Urethane thermoplastic elastomer (TPU)

Alternative and trade names
Elastollan®, Desmopan®, Estane®
Want to keep this datasheet? Save it now in your required format

Description

Thermoplastic block copolymer has high wear resistance, flexibility over a wide range of temperatures, and high elasticity over the entire hardness range. Resistance to weathering and high-energy radiation. The key features are:


  • Durable: High wear resistance and resistant to oils and some solvents.
  • Flexible: Functions over a high range of temperatures.
  • Versatile: Alter hardness, strength, rigidity, elasticity and cold-flexibility.
  • This material data has been provided by M-Base.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyValue

    Density

    1.05 - 1.34 g/cm³

    Show Material materials with Density of 1.05 - 1.34 g/cm³

    Mechanical

    PropertyValueComment

    Elastic modulus

    0.03 - 0.7 GPa

    Show Material materials with Elastic modulus of 0.03 - 0.7 GPa

    Elongation

    350.0 - 800.0 %

    Show Material materials with Elongation of 350.0 - 800.0 %

    Tensile strength

    20.0 - 60.0 MPa

    Show Material materials with Tensile strength of 20.0 - 60.0 MPa

    at 350-800% strain

    Impact strength, Charpy notched

    no break

    Impact strength, Charpy unnotched

    no break

    Thermal

    PropertyValue

    Coefficient of thermal expansion

    0.00011 - 0.00017 1/K

    Show Material materials with Coefficient of thermal expansion of 0.00011 - 0.00017 1/K

    Melting point

    120.0 - 220.0 °C

    Show Material materials with Melting point of 120.0 - 220.0 °C

    Specific heat capacity

    1500.0 - 1700.0 J/(kg·K)

    Show Material materials with Specific heat capacity of 1500.0 - 1700.0 J/(kg·K)

    Thermal conductivity

    0.14 - 0.5 W/(m·K)

    Show Material materials with Thermal conductivity of 0.14 - 0.5 W/(m·K)

    Flammability

    UL 94 HB

    Electrical

    PropertyValue

    Dielectric constant

    4 [-]

    Show Material materials with Dielectric constant of 4 [-]

    7 [-]

    Show Material materials with Dielectric constant of 7 [-]

    Electrical resistivity

    1000000000.0 - 1000000000000.0 Ω·m

    Show Material materials with Electrical resistivity of 1000000000.0 - 1000000000000.0 Ω·m

    Optical

    PropertyValue

    Transparency

    yes

    Technological properties

    Property
    Application areas

    Damping elements, ear tags, cable sheathing, Winter Sports Equipment

    Processing methods

    Injection molding, blow molding, extrusion, coating