General
Property | Value |
---|---|
Density | 1.0 - 1.15 g/cm³ Show Material materials with Density of 1.0 - 1.15 g/cm³ |
Mechanical
Property | Value | Comment | |
---|---|---|---|
Elastic modulus | 0.07 - 0.51 GPa Show Material materials with Elastic modulus of 0.07 - 0.51 GPa | ||
Elongation | 300.0 - 700.0 % Show Material materials with Elongation of 300.0 - 700.0 % | ||
Impact strength, Charpy notched | 15 kJ/m² Show Material materials with Impact strength, Charpy notched of 15 kJ/m² | no break | |
Tensile strength | 10.0 - 40.0 MPa Show Material materials with Tensile strength of 10.0 - 40.0 MPa | at 15-30% strain | |
Impact strength, Charpy unnotched | no break |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 0.00014 - 0.00021 1/K Show Material materials with Coefficient of thermal expansion of 0.00014 - 0.00021 1/K |
Melting point | 135.0 - 210.0 °C Show Material materials with Melting point of 135.0 - 210.0 °C |
Flammability | UL 94 HB |
Electrical
Property | Value |
---|---|
Dielectric constant | 5 [-] Show Material materials with Dielectric constant of 5 [-] |
10 [-] Show Material materials with Dielectric constant of 10 [-] | |
Electrical resistivity | 100000000.0 - 300000000.0 Ω·m Show Material materials with Electrical resistivity of 100000000.0 - 300000000.0 Ω·m |
Optical
Property | Value |
---|---|
Transparency | yes |
Technological properties
Property | ||
---|---|---|
Application areas | Catheters, shoe components, mantle layers for golfballs, air ducts | |
Other | You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application: Polymer Advanced Search | |
Processing methods | Injection molding, blow molding, extrusion, transfer molding, casting, thermoforming |