Styrenic thermoplastic elastomer (TPS)

Alternative and trade names
Evoprene®, OnFlex™, PHOENIX™
Want to keep this datasheet? Save it now in your required format

Description

These compounds have rubber-like properties, yet flow like thermoplastics when exposed to heat and pressure. TPE-S based products are characterized by low compression set and good resistance to various media. Special types with adhesion properties to various thermoplastics complement the portfolio. The main features are:


  • Chemical Resistance (Ozone and cleaning agents)
  • Excellent weatherability
  • Good tear resistance
  • This material data has been provided by M-Base.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyValue

    Density

    0.88 - 1.24 g/cm³

    Show Material materials with Density of 0.88 - 1.24 g/cm³

    Mechanical

    PropertyValue

    Elongation

    300.0 - 1800.0 %

    Show Material materials with Elongation of 300.0 - 1800.0 %

    Tensile strength

    at 300-1800% strain

    Thermal

    PropertyValue

    Flammability

    UL 94 HB

    Optical

    PropertyValue

    Transparency

    yes

    Technological properties

    Property
    Application areas

    Shoe solings, houseware grips, air bag covers, gaskets, pen grips

    Other

    You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application:

    Polymer Advanced Search

    Processing methods

    Injection molding, blow molding, extrusion, calandering, coating, compression molding