General Polyurethane, rigid foams (PUR-R)

.XLSX
.PDF
Save

Properties

General

Density ρ

0.03 - 0.09 g/cm³ at 20 °C

Mechanical

Elongation A

4 - 5 % at 20 °C

Max allowed stress σmax

0.2 - 0.9 MPa at 20 °C

at 4-5% strain

Thermal

Thermal conductivity λ

0.02 - 0.03 W/(m·K) at 20 °C

Optical

Transparency

no

Technological properties

Application areas

Insulation applications, automotive interiors

Fillers

Unfilled, no additives.

Processing methods

Foaming

This material data has been provided by M-Base.