Polyurethane, rigid foams (PUR-R)

Want to keep this datasheet? Save it now in your required format

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

0.03 - 0.09 g/cm³

Show Material materials with Density of 0.03 - 0.09 g/cm³

Mechanical

PropertyValueComment

Elongation

4.0 - 5.0 %

Show Material materials with Elongation of 4.0 - 5.0 %

Tensile strength

0.2 - 0.9 MPa

Show Material materials with Tensile strength of 0.2 - 0.9 MPa

at 4-5% strain

Thermal

PropertyValue

Thermal conductivity

0.02 - 0.03 W/(m·K)

Show Material materials with Thermal conductivity of 0.02 - 0.03 W/(m·K)

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

Insulation applications, automotive interiors

Processing methods

Foaming