Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 120 - 156 GPa Show Material materials with Elastic modulus of 120 - 156 GPa | Typical for Cast Copper Nickel Grade |
Poisson's ratio | 23.0 °C | 0.34 [-] Show Material materials with Poisson's ratio of 0.34 [-] | Typical for Cast Copper Nickel Grade |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.8E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.8E-5 1/K | Typical for Cast Copper Nickel Grade |
Melting point | 1100 - 1240 °C Show Material materials with Melting point of 1100 - 1240 °C | Typical for Cast Copper Nickel Grade | |
Specific heat capacity | 23.0 °C | 377 J/(kg·K) Show Material materials with Specific heat capacity of 377 J/(kg·K) | Typical for Cast Copper Nickel Grade |
Thermal conductivity | 23.0 °C | 23 - 45 W/(m·K) Show Material materials with Thermal conductivity of 23 - 45 W/(m·K) | Typical for Cast Copper Nickel Grade |
Chemical properties
Property | Value |
---|---|
Aluminium | 5E-3 % Show Material materials with Aluminium of 5E-3 % |
Copper | 65 - 67 % Show Material materials with Copper of 65 - 67 % |
Iron | 0.25 - 1 % Show Material materials with Iron of 0.25 - 1 % |
Lead | 5E-3 % Show Material materials with Lead of 5E-3 % |
Manganese | 0.8 - 1.5 % Show Material materials with Manganese of 0.8 - 1.5 % |
Nickel | 29.5 - 31.5 % Show Material materials with Nickel of 29.5 - 31.5 % |
Phosphorus | 0.02 % Show Material materials with Phosphorus of 0.02 % |
Silicon | 0.3 - 0.5 % Show Material materials with Silicon of 0.3 - 0.5 % |
Sulfur | 0.02 % Show Material materials with Sulfur of 0.02 % |