Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 100 - 125 GPa Show Material materials with Elastic modulus of 100 - 125 GPa | Typical for Wrought Copper Brass |
Elongation A50 | 23.0 °C | 20 % Show Material materials with Elongation A50 of 20 % | |
Shear modulus | 23.0 °C | 40 GPa Show Material materials with Shear modulus of 40 GPa | Typical for Wrought Copper Brass |
Tensile strength | 23.0 °C | 380 MPa Show Material materials with Tensile strength of 380 MPa | |
Yield strength Rp0.5 | 23.0 °C | 150 MPa Show Material materials with Yield strength Rp0.5 of 150 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.7E-5 - 2.1E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.7E-5 - 2.1E-5 1/K | Typical for Wrought Copper Brass |
Melting point | 875 - 1075 °C Show Material materials with Melting point of 875 - 1075 °C | Typical for Wrought Copper Brass | |
Specific heat capacity | 23.0 °C | 371 - 418 J/(kg·K) Show Material materials with Specific heat capacity of 371 - 418 J/(kg·K) | Typical for Wrought Copper Brass |
Thermal conductivity | 23.0 °C | 100 - 234 W/(m·K) Show Material materials with Thermal conductivity of 100 - 234 W/(m·K) | Typical for Wrought Copper Brass |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.25 % Show Material materials with Aluminium of 0.25 % |
Copper | 57 - 60 % Show Material materials with Copper of 57 - 60 % |
Iron | 0.8 - 2 % Show Material materials with Iron of 0.8 - 2 % |
Lead | 0.2 % Show Material materials with Lead of 0.2 % |
Manganese | 0.05 - 0.5 % Show Material materials with Manganese of 0.05 - 0.5 % |
Tin | 0.5 - 1.5 % Show Material materials with Tin of 0.5 - 1.5 % |