Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 96 - 120 GPa Show Material materials with Elastic modulus of 96 - 120 GPa | Typical for Cast Copper Bronze |
Elongation A50 | 23.0 °C | 20 % Show Material materials with Elongation A50 of 20 % | |
Poisson's ratio | 23.0 °C | 0.34 [-] Show Material materials with Poisson's ratio of 0.34 [-] | Typical for Cast Copper Bronze |
Tensile strength | 23.0 °C | 620 MPa Show Material materials with Tensile strength of 620 MPa | |
Yield strength Rp0.5 | 23.0 °C | 275 MPa Show Material materials with Yield strength Rp0.5 of 275 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.6E-5 - 1.9E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.6E-5 - 1.9E-5 1/K | Typical for Cast Copper Bronze |
Melting point | 760 - 1060 °C Show Material materials with Melting point of 760 - 1060 °C | Typical for Cast Copper Bronze | |
Specific heat capacity | 23.0 °C | 376 - 440 J/(kg·K) Show Material materials with Specific heat capacity of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Thermal conductivity | 23.0 °C | 12 - 81 W/(m·K) Show Material materials with Thermal conductivity of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Chemical properties
Property | Value |
---|---|
Aluminium | 7 - 8.5 % Show Material materials with Aluminium of 7 - 8.5 % |
Copper | 71 % Show Material materials with Copper of 71 % |
Iron | 2 - 4 % Show Material materials with Iron of 2 - 4 % |
Lead | 0.03 % Show Material materials with Lead of 0.03 % |
Manganese | 11 - 14 % Show Material materials with Manganese of 11 - 14 % |
Nickel | 1.5 - 3 % Show Material materials with Nickel of 1.5 - 3 % |
Silicon | 0.1 % Show Material materials with Silicon of 0.1 % |