Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 96 - 120 GPa Show Material materials with Elastic modulus of 96 - 120 GPa | Typical for Cast Copper Bronze |
Elongation A50 | 23.0 °C | 13 % Show Material materials with Elongation A50 of 13 % | |
Poisson's ratio | 23.0 °C | 0.34 [-] Show Material materials with Poisson's ratio of 0.34 [-] | Typical for Cast Copper Bronze |
Tensile strength | 23.0 °C | 650 MPa Show Material materials with Tensile strength of 650 MPa | |
Yield strength Rp0.2 | 23.0 °C | 270 MPa Show Material materials with Yield strength Rp0.2 of 270 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.6E-5 - 1.9E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.6E-5 - 1.9E-5 1/K | Typical for Cast Copper Bronze |
Melting point | 760 - 1060 °C Show Material materials with Melting point of 760 - 1060 °C | Typical for Cast Copper Bronze | |
Specific heat capacity | 23.0 °C | 376 - 440 J/(kg·K) Show Material materials with Specific heat capacity of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Thermal conductivity | 23.0 °C | 12 - 81 W/(m·K) Show Material materials with Thermal conductivity of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Chemical properties
Property | Value |
---|---|
Aluminium | 9 - 10 % Show Material materials with Aluminium of 9 - 10 % |
Copper | 77.5 % Show Material materials with Copper of 77.5 % |
Iron | 4 - 5 % Show Material materials with Iron of 4 - 5 % |
Lead | 0.02 % Show Material materials with Lead of 0.02 % |
Manganese | 1.5 % Show Material materials with Manganese of 1.5 % |
Nickel | 4.5 - 5.8 % Show Material materials with Nickel of 4.5 - 5.8 % |
Silicon | 0.1 % Show Material materials with Silicon of 0.1 % |