Property | Value |
---|---|
Aluminium | 9 - 11 % Show Material materials with Aluminium of 9 - 11 % |
Iron | 2 - 4 % Show Material materials with Iron of 2 - 4 % |
Manganese | 1.5 % Show Material materials with Manganese of 1.5 % |
Nickel | 4 - 5.5 % Show Material materials with Nickel of 4 - 5.5 % |
Silicon | 0.25 % Show Material materials with Silicon of 0.25 % |
Tin | 0.2 % Show Material materials with Tin of 0.2 % |
Zinc | 0.3 % Show Material materials with Zinc of 0.3 % |