General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 7.7 - 8.7 g/cm³ Show Material materials with Density of 7.7 - 8.7 g/cm³ | Typical for Leaded Phosphor Bronze |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 110 - 130 GPa Show Material materials with Elastic modulus of 110 - 130 GPa | Typical for Leaded Phosphor Bronze |
Elongation A50 | 23.0 °C | 6 % Show Material materials with Elongation A50 of 6 % | |
Hardness, Rockwell C | 23.0 °C | 26 [-] Show Material materials with Hardness, Rockwell C of 26 [-] | |
Poisson's ratio | 23.0 °C | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Leaded Phosphor Bronze |
Tensile strength | 23.0 °C | 890 - 930 MPa Show Material materials with Tensile strength of 890 - 930 MPa | |
Yield strength Rp0.5 | 23.0 °C | 620 - 690 MPa Show Material materials with Yield strength Rp0.5 of 620 - 690 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.5E-5 - 1.9E-5 1/K | Typical for Leaded Phosphor Bronze |
Specific heat capacity | 23.0 °C | 380 J/(kg·K) Show Material materials with Specific heat capacity of 380 J/(kg·K) | Typical for Leaded Phosphor Bronze |
Chemical properties
Property | Value |
---|---|
Aluminium | 10 - 11 % Show Material materials with Aluminium of 10 - 11 % |
Copper | 74.5 % Show Material materials with Copper of 74.5 % |
Iron | 4 - 5.5 % Show Material materials with Iron of 4 - 5.5 % |
Lead | 0.03 % Show Material materials with Lead of 0.03 % |
Manganese | 1.5 % Show Material materials with Manganese of 1.5 % |
Nickel | 4.2 - 6 % Show Material materials with Nickel of 4.2 - 6 % |
Tin | 0.25 % Show Material materials with Tin of 0.25 % |
Zinc | 0.3 % Show Material materials with Zinc of 0.3 % |