Mechanical
Property | Temperature | Value |
---|---|---|
Elongation A50 | 20.0 °C | 15 % Show Material materials with Elongation A50 of 15 % |
Tensile strength | 20.0 °C | 620 MPa Show Material materials with Tensile strength of 620 MPa |
Yield strength Rp0.5 | 20.0 °C | 275 - 345 MPa Show Material materials with Yield strength Rp0.5 of 275 - 345 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 8.7 - 9.5 % Show Material materials with Aluminium of 8.7 - 9.5 % |
Iron | 3.5 - 4.3 % Show Material materials with Iron of 3.5 - 4.3 % |
Lead | 0.02 % Show Material materials with Lead of 0.02 % |
Manganese | 1.2 - 2 % Show Material materials with Manganese of 1.2 - 2 % |
Nickel | 4 - 4.8 % Show Material materials with Nickel of 4 - 4.8 % |
Silicon | 0.1 % Show Material materials with Silicon of 0.1 % |